不锈钢冶炼渣熔融还原及毒性浸出实验研究 被引量:8

SMELTING REDUCTION OF SLAG FROM STAINLESS STEELMAKING AND THE TOXICITY LEACHING TEST
下载PDF
导出
摘要 通过半工业化试验证实了可以通过铁浴熔融还原工艺快速回收不锈钢冶炼渣中的铬。采用X射线衍射分析、荧光分析和化学分析方法,得到不锈钢渣的初始成分及物相,熔融还原处理后熔渣中Cr最优收得率达到98.6%,渣中残铬量最低可降至0.063%。并根据相关标准进行了毒性浸出试验,确认了不锈钢冶炼渣经过处理,浸出毒性从0.62 mg/L降低至0.017 86 mg/L,远远低于一般废弃物的标准。 Smelting reduction process of stainless steelmaking slag was verified in semi-industrial test,which showed that reduction rate of Cr increased up to 98.6% in 20 min.The initial composition and phase composition of stainless steel slag were analyzed by the methods of XRD、XRF and chemical analysis.The content of residual Cr in slag was decreased down to 0.063%,whose results of toxicity leaching test was 0.017 86 mg/L and far less than the environmental standards.
出处 《上海金属》 CAS 2011年第4期44-47,共4页 Shanghai Metals
基金 国家自然科学基金(50634040)
关键词 不锈钢冶炼渣 熔融还原 残余铬含量 毒性浸出 Stainless Steelmaking Slag Smelting Reduction Residual Chromium Content Toxicity Leaching
  • 相关文献

参考文献13

二级参考文献24

  • 1刘大银,周才鑫,唐秋泉,彭易正,王献,董方刚,叶继雄.铬渣烧结矿炼制含铬生铁工业化生产试验研究[J].环境科学,1994,15(5):31-34. 被引量:14
  • 2侯树庭,徐明华,张怀,杨兴林,徐匡迪,蒋国昌,徐建伦,张晓兵.15吨铁浴熔融还原工业性试验[J].钢铁,1995,30(8):16-21. 被引量:11
  • 3马书文.铬渣治理与资源化综述[J].无机盐工业,1997,11(2):19-22. 被引量:17
  • 4Takamitsu Nakasuga. Reduction Rate of Cr2O3 in a Solid Powder State and in CaO-SiO2-M, O3-CaF2 Slags by Fe-C-Si Melts [J], ISIJ, 2001, (41): 937-9d4.
  • 5Takamitsu Nakasuga. Recovery Rate of Chromium from Stainless Slag by Iron Melts [J], ISIJ International, 2004, (44) : 665 - 672.
  • 6梁连科 车荫昌 杨怀 等.冶金热力学及动力学[M].沈阳:东北工学院出版社,1990..
  • 7工业固体废物采样制样技术规范HJ/T20-1998.
  • 8危险废物浸出毒性浸出方法标准-水平振荡浸出程序GB5086.1-1997.
  • 9肖艳萍.熔融还原的基础研究[D].沈阳:东北大学,1988.
  • 10片山博,宮内克行,出倉直樹,ほか.予僃還元クロム鉱石の溶融還元挙動[J].铁と鋼,1993,79(6):34-40.

共引文献62

同被引文献64

引证文献8

二级引证文献19

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部