摘要
研究了TiVCr合金的有效储氢量CH与电负性差、原子尺寸参数和外层电子数之间的定量关系,可表示为:TlnCH=0.45922T+5044.8(?X)2+1250.6δ2-285.80n2/3。外层电子数因数对TiVCr合金的CH影响最大,电负性差因数对CH影响最小。当n2/3值在1.98和2.14之间、δ2值在0.255和0.288之间、(?X)2值在0.0638和0.0765之间时,TiVCr合金的有效储氢量大于2.0wt%。
The relation between the effective hydrogen storage capacity CH of Ti-V-Cr alloys and out-layer electrons,atomic diameter difference,electronegativity difference has been studied.It is shown that their relation can be expressed as TlnCH = 0.45922T+5044.8(X)2+1250.6δ2-285.80 n2/3.The factor of out-layer electrons has the largest effect on the CH of Ti-V-Cr alloys,while the factor of electronegativity difference has the smallest effect among the three bond parameters.The effective hydrogen storage capacity of Ti-V-Cr alloys is greater than 2.0wt% when n2/3 values of Ti-V-Cr alloys are between 1.98 and 2.14,2 values are between 0.255 and 0.288 and(X) 2 values are between 0.0638 and 0.0765.
出处
《稀有金属材料与工程》
SCIE
EI
CAS
CSCD
北大核心
2011年第7期1152-1156,共5页
Rare Metal Materials and Engineering
基金
Shanghai Municipal Commission of Science and Technology (075211019)
关键词
储氢量
TiVCr合金
电负性差
原子尺寸参数
外层电子数
hydrogen storage capacity
TiVCr alloys
electronegativity difference
atomic size parameters
out-layer electrons