摘要
对陶瓷工业废料及粉煤灰生产再生陶瓷墙地砖进行了研究,并引入少量硼砂作为助熔剂,使工业废料总利用率达25%~35%,再生陶瓷制品强度提高幅度达16.4%-35%。
It was studied in the article that ceramic industrial waste and fly ash was used to produce recycle ceramic brick.By using little borax as flux,using percent of industrial waste reached 25%~35% and strength of the product was improved at 16.4%~35%.
出处
《粉煤灰综合利用》
CAS
2011年第4期7-9,共3页
Fly Ash Comprehensive Utilization
基金
湖南省教育厅资助项目(项目编号:10K026)
关键词
陶瓷
工业废料
粉煤灰
硼砂
ceramic
industrial waste
fly ash
borax