期刊文献+

新型无熟料矿渣水泥的试验研究 被引量:9

Experimental Study on the New Non-clinker Slag Cement
下载PDF
导出
摘要 以高炉矿渣为主要原料,添加Ca(OH)2、CaCO3、可溶性钙盐等辅助材料可在pH值较低的条件下制备出一种不需煅烧的无熟料水泥,该水泥中矿渣掺量可达80%,强度可达国标42.5级水泥要求。Ca(OH)2、CaCO3可以激发矿渣的活性,可溶性钙盐的加入降低了水泥的pH值,进一步激发了矿渣的活性。其主要水化产物为C-S-H凝胶和水化碳铝酸钙。 The Non-clinker cement with lower pH was prepared with blast furnace slag as the main raw material, and Ca( OH)2, CaCO3, soluble calcium salts as support materials. The slag in the cement reached up to 80% and the Non-clinker cement meets the requirements for strength class 42.5. Ca(OH) 2 combined with CaCO3 stimulate the activity of slag, which was further stimulated by lowering the pH values by the addition of soluble calcium salts. The main hydration products were the carbon-calcium aluminate and C-S-H gel.
出处 《硅酸盐通报》 CAS CSCD 北大核心 2011年第4期920-924,共5页 Bulletin of the Chinese Ceramic Society
关键词 矿渣 无熟料水泥 PH值 slag non-clinker cement pH value
  • 相关文献

参考文献6

二级参考文献18

  • 1郑娟荣,覃维祖,张涛.碱-偏高岭土胶凝材料的凝结硬化性能研究[J].湖南大学学报(自然科学版),2004,31(4):60-63. 被引量:42
  • 2施惠生.土聚水泥制备的探索试验与研究[J].水泥技术,2005(4):15-18. 被引量:16
  • 3史才军.碱-激发水泥混凝土研究中的一些误区和挑战[A].第二界全国化学激发胶凝材料研讨会论文集[c],西安建筑科技大学,2007.
  • 4廖佳庆,杨长辉,陈科.碱矿渣水泥化学收缩研究[A].第二界全国化学激发胶凝材料研讨会论文集[c],西安建筑科技大学,2007.
  • 5Trettin R. Reactivity and mechanism of hydration of cement phases [ A ]. Proceeding of the 11 th International Congress on the Chemistry of Cement [ C ] , Gothenburg, Sweden, 1997.
  • 6Xua H, Van Deventer J S J. The geopolymerisation of alumino-silicate minerals[ J]. Int. J. Miner. Process. ,2000,59:247-266.
  • 7Palomo A ,Glasser F F. Chemically-bonded cementitious materials based on metakaolin[ J]. Br. Ceram. Trans. J. , 1992,91:107-112.
  • 8李东旭.低钙玻璃态碱胶凝材料的研究进展[A].第一届全国化学激发剂材料研讨会论文集[C].南京:南京工业大学出版社,2004.30-40.
  • 9社团法人.セメント协会.C&Cェンサイヮロペヂイヅ[M].セメント协会,1996.114.
  • 10笠井芳夫.セメント·コンクリ一ト用混合材料[M].改订版.技术书院,1986.39-40.