摘要 The reduction degradation characteristics of typical sinter, pellet and lump ore were tested with the reducing gas conditions simulating two kinds of irowmaking processes. The results show that, in the same condition of gas composition and temperature, the reduction degradation degree (RDI〈3.15mm) of sinter is high, RDI〈3.15mm of lump ore is low and RDI〈3.15 mm of pellet is in the middle level. With two kinds of gas composition simulating different iron-making processes, the reduction degradation indices (RDI) of three kinds of iron ores all present the tenden- cy of "inverted V-shape" in the temperature range from 450 to 650℃, and the RDI reach the maximum value at 550℃. The reduction degradation degrees of iron ores are extended when mixing the gas with hydrogen to increase the re duction potential, and the influence extent is discrepant for different iron ores. Colligating the increase amplitude of grains in small size fraction, the influence of reducing gas on lump ore is the greatest, the influence on sinter is the second, and the sensitivity of pellet on the reducing gas properties change is relatively small. As for the degradation form, lump ore and sinter both present the degradation ,of cracking, and the distribution of small grains generated from the cracking is in the range from 03 5 to 6. 3 mm uniformly. The lump ore presents surface cracking, while sin- ter presents integral cracking. The pellet presents the degradation of surface stripping, and the proportion of grains smaller than 0.5 mm is the highest, which is up to 90% in the grains smaller than 3.15 mm. The reduction degradation characteristics of typical sinter, pellet and lump ore were tested with the reducing gas conditions simulating two kinds of irowmaking processes. The results show that, in the same condition of gas composition and temperature, the reduction degradation degree (RDI〈3.15mm) of sinter is high, RDI〈3.15mm of lump ore is low and RDI〈3.15 mm of pellet is in the middle level. With two kinds of gas composition simulating different iron-making processes, the reduction degradation indices (RDI) of three kinds of iron ores all present the tenden- cy of "inverted V-shape" in the temperature range from 450 to 650℃, and the RDI reach the maximum value at 550℃. The reduction degradation degrees of iron ores are extended when mixing the gas with hydrogen to increase the re duction potential, and the influence extent is discrepant for different iron ores. Colligating the increase amplitude of grains in small size fraction, the influence of reducing gas on lump ore is the greatest, the influence on sinter is the second, and the sensitivity of pellet on the reducing gas properties change is relatively small. As for the degradation form, lump ore and sinter both present the degradation ,of cracking, and the distribution of small grains generated from the cracking is in the range from 03 5 to 6. 3 mm uniformly. The lump ore presents surface cracking, while sin- ter presents integral cracking. The pellet presents the degradation of surface stripping, and the proportion of grains smaller than 0.5 mm is the highest, which is up to 90% in the grains smaller than 3.15 mm.
出处 《Journal of Iron and Steel Research(International)》 SCIE EI CAS CSCD 2011年第8期20-24,共5页 钢铁研究学报(英文版)
关键词 SINTER PELLET lump ore low temperature reduction degradation characteristic gas property sinter pellet lump ore low temperature reduction degradation characteristic gas property
  • 相关文献

参考文献3

共引文献27

同被引文献112

引证文献12

二级引证文献54

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部