摘要
本文研究了在相同退火热处理条件下,不同析出相含量的两种铝镁合金5456和5052在不同加载应变率下的P-LC效应.结果表明析出相对两种材料的P-LC效应有明显影响,并且析出相含量的不同所产生的影响不同.此外,析出相含量较少的5052合金的溶质原子的扩散方式是管扩散,而析出相含量较多的5456合金不再局限于管扩散的方式,而是更为复杂.
In the alloy with solute content higher than the limiting solubility, the solute atoms failing to dissolve will precipitate from the solid solution and form precipitations. In this study, the Portevin-Le Chatelier (P-LC) effects in annealed 5456 and 5052 aluminum alloys with different precipitation content are investigated under different applied strain rates respectively. The findings suggest that precipitations have a significant effect on the P-LC effect and different precipitation content has different effects. Furthermore, the solute diffusion is pipe diffusion in 5052 alloy with lower precipitation content. However, for 5456 alloy with higher precipitation content, the diffusion is no longer the case but more complex.
出处
《物理学报》
SCIE
EI
CAS
CSCD
北大核心
2011年第9期514-521,共8页
Acta Physica Sinica
基金
国家自然科学基金(批准号:10732080
10872189)资助的课题~~