1Bagby M,Marshall ST,Marshall GW.Metal ceramic compatibility:Areview of the literature.J Prosthet Dent,1990,63(1):21.
2Derand T.Residual stress in metal-ceramic crowns.J Oral Rehabil,1981,8(1):69-74.
3Asaoka K,Tesk JA.Transieny and residual stress in porcelain metal strip[J].J Dent Res,1990,69.463-468.
4Carpenter MA,Goodkind RJ.Effect of varying surface texture on bondstrength of one semiprecious and one nonprecious ceramo-alloy.J Pros-thet Dent,1979,42(1):86.
5Warpehe WS,Goodkind RJ.Design and technique variables affectingfracture resistance of metal-ceramic restorations.J Prosthet Dent,1976.
7Wu Y,Moser JB,Jameson LM,et al.The effect of oxidation heat treat-ment on porcelain bond strength in selected base metal alloys.J ProsthetDent,1991,66(4):439.
8MegerT.Chemical bonding in the porcelain-baked-metal technique.J Dent Res,1971,50(3):760.