摘要 为了给大规模合理开发本钢集团贾家堡子铁矿8号矿体矿石资源提供技术依据,针对该矿石磁铁矿嵌布粒度微细的特点,采用大块干式磁选抛废—单一弱磁选和大块干式磁选抛废—弱磁选—反浮选两种工艺流程进行了选矿试验。结果表明:前者在-0.030 8 mm占90%的最终磨矿细度下,可获得铁品位为65.76%、回收率为75.93%的铁精矿;后者在-0.043 mm占90%的最终磨矿细度下,可获得铁品位为65.47%、回收率为74.43%的铁精矿。两流程技术指标相近,采用哪种流程取决于技术经济比较。 In order to provide technical basis for rationally developing mineral resources at No.8 ore-body of Benxi Iron and Steel Group in large-scale,and in view of the characteristics of micro-fine embedded magnetite,the beneficiation tests were carried by the process of bulk dry magnetic separation for tailings removal-single low intensity magnetic separation and the process of bulk dry magnetic separation-low intensity magnetic separation-reverse flotation.The results showed that iron concentrate with Fe grade of 65.76% and recovery of 75.93% was obtained by the former under the final grinding fineness-0.030 8 mm 90%;Iron concentrate with Fe grade of 65.47%,recovery of 74.43% was obtained by the latter under the grinding fineness of-0.043 mm 90%.Since the technical indexes obtained by the two processes are similar,which one you adopted depends on the technical and economical comparison.
作者 刘丽梅 张永
出处 《金属矿山》 CAS 北大核心 2011年第10期91-95,共5页 Metal Mine
关键词 贾家堡子铁矿8号矿体 微细粒嵌布磁铁矿 大块干式预选 弱磁选 反浮选 No.8 ore-body of Jiajiapuzi iron ore Micro-fine embedded magnetite Bulk dry concentration Low intensity magnetic separation Reverse flotation
  • 相关文献

参考文献3

  • 1张艳娇,刘广学,赵平,邵伟华,常学勇.贾家堡子微细粒磁铁矿选矿试验研究[J].金属矿山,2009,38(1):59-61. 被引量:8
  • 2张永.本溪钢铁(集团)公司贾家堡子铁矿八号矿体矿石单-弱磁选工艺流程试验研究报告[R].马鞍山:中钢集团马鞍山矿山研究院有限公司,2009.
  • 3樊绍良,张永.本溪钢铁(集团)公司贾家堡子铁矿八号矿体矿石磁选-反浮选工艺流程试验研究报告[R].马鞍山:中钢集团马鞍山矿山研究院有限公司,2009.

二级参考文献2

共引文献7

同被引文献6

引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部