摘要 通过红外测温和预防性试验发现罗店变电站的多只110 kV复合套氧化锌避雷器的绝缘性能有所下降,经解体试验和分析,认为原因是密封不良导致环氧筒受潮。指出红外测温能有效发现运行中的复合套氧化锌避雷器的此类缺陷。 It is found that the electrical insulation performance of many 110 kV polymer housed zinc oxide arrester degrades in Luodian Substation after the infrared temperature measurement and preventive tests.Cause analysis is performed after disassembly experiments.The reason is the undesirable sealing leading to epoxy tube affected by dampness.It indicates that the infrared temperature measurement is an effective method to detect this type of defect of the running zinc oxide arrester.
机构地区 金华电业局
出处 《浙江电力》 2011年第10期14-15,25,共3页 Zhejiang Electric Power
关键词 复合套氧化锌避雷器 红外测温 绝缘 受潮 polymer housed zinc oxide arrester infrared temperature measurement insulation damp
  • 相关文献

参考文献2

  • 1DL/T664-2008带电设备红外诊断技术应用规范[S].北京:中国电力出版社,2008.
  • 2Q/GDW168-2008输变电设备状态检修试验规程[S].北京:中围电力出版社,2008.

共引文献3

同被引文献40

引证文献5

二级引证文献20

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部