摘要
对低硫低铜磁铁矿进行了不同工艺研究, 采用先浮后磁和使用高选择性捕收剂可获得精矿含铁63 .18 % , 回收率84 .34 % , 含硫0 .38 % 的合格铁精矿; 含铜13 .83 % ,回收率51 .41 % 的铜精矿;含硫35 .19 % ,回收率73 .59 % 的硫精矿, 明显提高了矿产资源利用率。
In this paper the different technology separating low sulphur-low copper magnetite is researched.lt can obtain a lron concentrate of TFe 13.185 and S 0.38%with a recovery of 84.34%, a Copper concentrate of Cu 13.83%,with a recovery 51.41%and a Sulphur concentrate of S 35.19%,with a recovery 73.59%.The Utilization ratio of mineral resources is improved.
出处
《湖南有色金属》
CAS
1999年第5期9-11,38,共4页
Hunan Nonferrous Metals
关键词
低硫低铜磁铁矿
浮选-磁选流程
资源利用率
Low Sulphur-low copper magnetite, Preflotation-magnetic separating flow sheet, The utilixation ratio of mineral resources