Reduction behavior of preoxidized synthetic ilmenite was studied by means of Mossbauer spectra. In the course of reduction, iron component in the samples is reduced in stepwise: Fe 3+ →Fe 2+ →Fe 0, and some intermediate compounds, such as Fe 3O 4, Fe 2TiO 4 etc . and their solid solution may be generated besides Fe 2O 3 and FeTiO 3. If the reduction temperature is higher than 1173 K, the metallization needs only half time of the case when the temperature is lower than 1073 K.
Reduction behavior of preoxidized synthetic ilmenite was studied by means of Mossbauer spectra. In the course of reduction, iron component in the samples is reduced in stepwise: Fe 3+ →Fe 2+ →Fe 0, and some intermediate compounds, such as Fe 3O 4, Fe 2TiO 4 etc . and their solid solution may be generated besides Fe 2O 3 and FeTiO 3. If the reduction temperature is higher than 1173 K, the metallization needs only half time of the case when the temperature is lower than 1073 K.