摘要 It is showed that there are Ti 3Al, Ti 2Cu and β phase in the interface of Ti/Ti Al composites reinforced with Y 2O 3 Cr composite soft coated Ti fiber, and that interface bonding is intact. Bending strength of the composites can be increased by 26%, to 709 MPa, and bending deflection increased slightly compared with the Ti/Ti Al composites reinforced by Ti fibers coated with Y 2O 3. It is showed that there are Ti 3Al, Ti 2Cu and β phase in the interface of Ti/Ti Al composites reinforced with Y 2O 3 Cr composite soft coated Ti fiber, and that interface bonding is intact. Bending strength of the composites can be increased by 26%, to 709 MPa, and bending deflection increased slightly compared with the Ti/Ti Al composites reinforced by Ti fibers coated with Y 2O 3.
出处 《Rare Metals》 SCIE EI CAS CSCD 1997年第3期41-46,共6页 稀有金属(英文版)
关键词 Ti Al matrix composite Ti fiber Composite soft coating Mechanical property Ti Al matrix composite, Ti fiber, Composite soft coating, Mechanical property
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部