The phase transition behavior and aggregating states of [smectic LCP, PS(4BC/DM)/nematic LC, E7/chiral dopant, CB 15] ternary composite system were investigated on the basis of differential scanning calorimetry (DSC) measurement, polarizing optical microscopy (POM) observation and wide angle X ray diffraction (WAXD) patterns. It was demonstrated that if the weight ratio of the chiral dopant was fixed as 4.8wt%, an induced chiral nematic (N *) phase existed in the ternary system when PS(4BC/DM) ratio was below 47.6 wt%. Moreover, smectic like long range ordering appeared in the induced N * phase in a certain temperature range just above the smectic A(S A) N * phase transition when PS(4BC/DM) ratio was between 19.1wt% and 47.6wt%.
The phase transition behavior and aggregating states of [smectic LCP, PS(4BC/DM)/nematic LC, E7/chiral dopant, CB-15] ternary composite system were investigated on the basis of differential scanning calorimetry (DSC) measurement, polarizing optical microscopy (POM) observation and wide angle X-ray diffraction (WAXD) patterns. It was demonstrated that if the weight ratio of the chiral dopant was fixed as 4.8wt%, an induced chiral nematic (N^(*)) phase existed in the ternary system when PS(4BC/DM) ratio was below 47.6 wt%. Moreover, smectic like long range ordering appeared in the induced N^(*) phase in a certain temperature range just above the smectic A(S_(A))-N^(*) phase transition when PS(4BC/DM) ratio was between 19.1wt% and 47.6wt%.