摘要
CdS particles were generated in the mixed sodium 10- undecenoate--decyltrmethylammonium bromide vesicle dispersions.Depending on the condition and method of preparation. CdSsemi conductor absorption edges were found to range from 526 to 448 nm, corresponding to particle diameter between >5. 0 and 2. 7 nm.
CdS particles were generated in the mixed sodium 10- undecenoate--decyltrmethylammonium bromide vesicle dispersions.Depending on the condition and method of preparation. CdSsemi conductor absorption edges were found to range from 526 to 448 nm, corresponding to particle diameter between >5. 0 and 2. 7 nm.