摘要
Hamilton and ZHOU Shan-you reported that, because the high strength aluminium alloy 7075 contains more Fe and Si impurities than the high strength aluminium alloy 7475 does, its superplastic elongation is lower than the maximum elongation 1200% of 7475 aluminium alloy. ZHOU Shan-you has obtained the maximum elongation 500% of