摘要
文章以莱钢钢渣为原料,进行了湿式弱磁选回收铁的工艺试验研究和湿式磁选磨矿细度试验,所生产的铁精矿产率为31.08%,选矿比3.25,品位为61.30%,全铁回收率为68.21%。
The steel slag of Lai Steel was used as raw material in the paper.The technology of retrieving iron has been researched through wet low-intensity magnetic separation and low-intensity grinding fineness test.It showed that the result of wet low-intensity magnetic separation was superior,and iron concentrate was 31.08 %,concentration ratio was 3.25,grade was 61.30 %,total iron recovery was 68.21 %.
出处
《广东化工》
CAS
2011年第11期40-41,共2页
Guangdong Chemical Industry
关键词
钢渣
综合利用
磁选
铁精矿
steel slag
comprehensive utilization
magnetic dressing
iron concentrate