期刊文献+

储氢合金电极失效的机理分析及研究进展 被引量:3

Analysis and the Latest Research of Basic Mechanics on Efficacy Loss of Hydrogen Storage Alloy Electrode
下载PDF
导出
摘要 分析了储氢合金电极失效的四种基本理论,即合金颗粒粉化、元素氧化、吸氢非晶化与释氢晶化、电化学腐蚀机制,并综述其研究进展,提出延缓合金电极容量衰减,改善其循环性能的有效控制途径。 Analysis is made of the basic mechanics about efficacy loss of the electrode, such as pulverization of alloy particle, oxidation of element, amorphous after hydrogen absorption and crystalline after hydrogen desorption,and electrochemical corrosion. The latest research is reviewed. The way how to restrain or lower capacity degradation of electrode and improve cyclic property of hydrogen storage alloy electrode is introduced.
出处 《稀有金属与硬质合金》 CAS CSCD 北大核心 2011年第4期25-30,共6页 Rare Metals and Cemented Carbides
基金 国家863计划项目(2007AA03Z227 2007AA03Z230) 河北省自然科学基金(E2010000301) 河北大学自然科学研究计划项目(2009-152 2009-153) 河北大学大学生科技创新项目(2011071 2011073)
关键词 储氢合金 电极失效 容量衰减 循环性能 hydrogen storage alloy efficacy loss of electrode capacity degradation cyclic property
  • 相关文献

参考文献22

  • 1杨丽颖,董小平,耿晓光,王青,林玉芳,张羊换.稀土镁镍系合金的循环贮氢性能与粉化特性研究[J].粉末冶金工业,2011,21(2):19-24. 被引量:5
  • 2Liao B,Lei Y Q,Chen L X,et al. Effect of the La/Mg ratio on the structure and electrochemical properties of Lax Mg3-x Ni9 (co = 1.6 - 2.2) hydrogen storage electrode alloys for nickelmetal hydride batteries [J]. J Power Sources, 2004,129 (2) : 358-367.
  • 3.朱光潜美学文集(二)[M].上海:上海文艺出版社,1983.344-345.
  • 4周增林,宋月清,黄长庚,崔舜,张永健,李学军,黄倬.热处理对La_(0.7)Mg_(0.3)(Ni_(0.85)Co_(0.15))_(3.4)贮氢电极合金性能的影响[J].西安交通大学学报,2007,41(11):1373-1379. 被引量:6
  • 5Tanaka H, Senoh H, Kuriyama N, et al. Cycle durability of Ca-Mg-Ni alloys and factors which cause degradation of hydrogen storage capacity[J]. Materials Science and Engineering B,2004,108:81-90.
  • 6Liu Y F,Pan H G,Gao M X,et al. Function of Al on the cycling behavior of the La-Mg-Ni-Co-type alloy electrodes[J]. International Journal of Hydrogen Energy, 2008,33:124-133.
  • 7Dong X P, Zhang Y H, Lu F X, et al. Investigation on microstructures and electrochemical performances of La0.75 Mg0.25 Ni3.5 Cox (x = 0 - 0.6 ) hydrogen storage alloys [J]. International Journal of Hydrogen Energy, 2007,32(18) :4 949-4 956.
  • 8Liu Y F,Pan H G,Yue Y J,etal. Cycling durability and degradation behavior of La-Mg-Ni-Co-type metal hydride electrodes[J]. Journal of Alloys and Compounds, 2005, 395(1-2) :291-299.
  • 9Shang G Y,Han S M,Hao J S,etal. Study on self-discharge property of Nd0. 88 Mg0. 12 Ni3. 10 +x Al0. 20 (x = 0.00, 0.10,0. 20,0. 30) hydrogen storage alloys[J]. Journal of Alloys and Compounds,2010, 493: 573-576.
  • 10Wang Y Z, Zhao M S. Structure and electrochemical characteristics of Ti0.10 Zr0. 15 V0. 35 Cr0.10 Ni0. 30 -LaNi4 Al0. 4 Mn0. 3Co0.3 composite hydrogen storage alloy[J]. International Journal of Hydrogen Energy, 2010,35 (12) : 8 268-8 274.

二级参考文献38