期刊文献+

蚕丝制浆性能及其与针叶木浆配抄性能

Pulping Properties of Silk Fiber and Paper Furnished with Softwood Pulp
原文传递
导出
摘要 脱胶蚕丝经过碱液预浸渍后用PFI和盘磨打浆,并与针叶木浆配抄。对打浆后蚕丝的纤维形态及蚕丝与针叶木配抄后纸张的性能进行分析。结果表明,蚕丝经过处理后具有同植物纤维相近的分丝帚化性质;与针叶木浆配抄后,可以提高纸张的松厚度,添加量在10%时,可以提高纸张的抗张强度。 The degumed silk which was pretreated with dilute alkali solution was refined by PFI and disc refiner, and then used with softwood pulp. It was analyzed in this paper that the fiber morphology of the refined silk and the properties of paper made by silk fiber and softwood pulp. The results showed that silk fiber has the similar fibrous fibrillating property with plant fiber, the bulk of the paper made by silk fiber and softwood pulp can be improved and meanwhile when the addition of silk fiber is 10%, the paper tensile strength is improved.
出处 《纸和造纸》 北大核心 2011年第12期38-40,共3页 Paper and Paper Making
关键词 蚕丝 针叶木 松厚度 抗张强度 silk softwood bulk tensile strength
  • 相关文献

参考文献4

  • 1窦林名.冲击地压危险性评定的综合指数法[A]..2000高校洁净开采与支护技术研讨会[C].苏州,2000..
  • 2Kato Kiroshi. Adsorption properties of harmful gas by silk blended papersheets [J]. Journal of Sericulture Science of Japan, 2000, 69(5): 331.
  • 3李维贤,师严明,赵耀明.蚕丝纸的抄制及其性质[J].中国造纸学报,2003,18(1):66-69. 被引量:13
  • 4王建,王志杰,杨王贵.蚕丝制浆造纸性能初步探讨[J].中国造纸,2005,24(9):76-77. 被引量:4

二级参考文献16

  • 1Kato Kireshi.Adsorption properties of harmful gas by silk blended papersheets.J.Seric.Sci.Jpn.,2000,69(5):331.
  • 2Mucha M, Miskiewicz D. Chitosan blends as fillers for paper, Journal of Applied Polymer Science. 2000,77: 3210.
  • 3Kato Takeshi, Komurasaki Kazuhiko, Katayama Akira. Effects of chitosan treatment on the air permeability and heating resistance of silk fabrics. J. Seric. Sci .Jpn., 1996,65(2) : 128.
  • 4Hata Tamako, Kato Kiroshi. Fibrillation of silk fibers its treatment method and producing of silk paper. J.Seric. Sci .Jpn., 1997,66(2) : 132.
  • 5Kato Kiroshi.Properties ofthe handsheets made from heated silk fibers to fibfiate and regenerated cellulose apan fibels.J.Seric.Sci.Jpn.,1998,67(4):347.
  • 6Hata Tamako, Kato Kiroshi. Fibrillation of silk fibers, its treatment method and producing of silk paper[J]. J. seric. sci.jpn., 1997,66(2):132.
  • 7Kato Kiroshi. Adsorption properties of harmful gas by silk fibers to fibriate and regenerated cellulose apan fibers [J] .J.seric.sci.jpn.,1998,67(4) :347.
  • 8周宏湘.蚕丝差别化精练技术的进展[J].印染助剂,1997,14(3):1-5. 被引量:2
  • 9蔡彩凤.蚕丝的新用途[J].丝绸,1998,35(6):45-47. 被引量:9
  • 10曹丽云,黄剑锋,张光华.壳聚糖-丙烯酰胺接枝共聚物用作造纸增强、助留剂的研究[J].纸和造纸,2001,20(1):37-38. 被引量:11

共引文献13

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部