期刊文献+

Corrosion behavior of metals or alloys with a solid NaCl deposit in wet oxygen at medium temperature 被引量:4

Corrosion behavior of metals or alloys with a solid NaCl deposit in wet oxygen at medium temperature
原文传递
导出
摘要 The corrosion of metals or alloys under solid NaCl deposit in wet oxygen (water vapor and oxygen) at medium temperature 4013-700℃ causes serious damage and has received considerable attention in recent years. Series of mechanistic studies have revealed synergistic interactions between solid NaCl and water vapor, which accelerates the corrosion process. In addition, the overall corrosion process comprises both chemical reactions (oxidation) and electrochemical reactions and their mutual inter- actions depend on the system of interest. Interestingly, the wet oxygen environment was found to modify the reactions of the element Cr, which plays a useful role in corrosion protection in this special environment.
出处 《Science China(Technological Sciences)》 SCIE EI CAS 2012年第2期369-376,共8页 中国科学(技术科学英文版)
基金 supported by the National Natural Science Fundation of China (Grant Nos. 50671113 and 50801063)
关键词 synergistic effect NaCl deposit water vapor electrochemical reactions 腐蚀行为 介质温度 盐矿床 氧气 合金 金属 电化学反应 腐蚀过程
  • 相关文献

参考文献20

  • 1C. Wang,F. Jiang,F. Wang.Corrosion Inhibition of 304 Stainless Steel by Nano-Sized Ti/Silicone Coatings in an Environment Containing NaCl and Water Vapor at 400–600°C[J].Oxidation of Metals (-).2004(1-2)
  • 2F. Wang,Y. Shu.Influence of Cr Content on the Corrosion of Fe–Cr Alloys: The Synergistic Effect of NaCl and Water Vapor[J].Oxidation of Metals (-).2003(3-4)
  • 3Fuhui Wang,Shujiang Geng,Shenglong Zhu.Corrosion Behavior of a Sputtered K38G Nanocrystalline Coating with a Solid NaCl Deposit in Wet Oxygen at 600 to 700°C[J].Oxidation of Metals (-).2002(1-2)
  • 4S. Geng,F. Wang,S. Zhu,W. Wu.Hot-Corrosion Resistance of a Sputtered K38G Nanocrystalline Coating in Molten Sulfate at 900°C[J].Oxidation of Metals (-).2002(5-6)
  • 5Shujiang Geng,Fuhui Wang,Shenglong Zhu.High-Temperature Oxidation Behavior of Sputtered IN 738 Nanocrystalline Coating[J].Oxidation of Metals (-).2002(3-4)
  • 6Yonghua Shu,Fuhui Wang,Weitao Wu.Corrosion Behavior of Pure Cr with a Solid NaCl Deposit in O2 Plus Water Vapor[J].Oxidation of Metals (-).2000(5-6)
  • 7H. Asteman,J.-E. Svensson,M. Norell,L.-G. Johansson.Influence of Water Vapor and Flow Rate on the High-Temperature Oxidation of 304L; Effect of Chromium Oxide Hydroxide Evaporation[J].Oxidation of Metals (-).2000(1-2)
  • 8Yonghua Shu,Fuhui Wang,Weitao Wu.Corrosion Behavior of Ti60 Alloy Coated with a Solid NaCl Deposit in O2 Plus Water Vapor at 500-700°C[J].Oxidation of Metals (-).1999(5-6)
  • 9H. Asteman,J.-E. Svensson,L.-G. Johansson,M. Norell.Indication of Chromium Oxide Hydroxide Evaporation During Oxidation of 304L at 873 K in the Presence of 10% Water Vapor[J].Oxidation of Metals (-).1999(1-2)
  • 10Yonghua Shu,Fuhui Wang,Weitao Wu.Synergistic Effect of NaCl and Water Vapor on the Corrosion of 1Cr-11Ni-2W-2Mo-V Steel at 500-700°C[J].Oxidation of Metals (-).1999(1-2)

同被引文献37

引证文献4

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部