退火工艺对锻态铁基合金组织性能的影响
摘要
以50%锻造态的FeCr2.2C1.92M合金为原料,对其进行合理的退火处理,通过金相观察和硬度测试,研究退火温度及保温时间对其组织性能的影响,并探索其最佳退火工艺制度。
出处
《内蒙古科技与经济》
2012年第1期103-104,共2页
Inner Mongolia Science Technology & Economy
参考文献5
-
1陈畅,汪明朴,金鹏,张娟,郭明星,谭望.退火温度对镦粗纯钼棒组织和横向塑性的影响[J].中国有色金属学报,2009,19(6):1061-1067. 被引量:12
-
2R. Lindau, A. Moslang, M. Schirra, et al. Mechanical and microstructural properties of a hipped RAFM ODS- steel [J]. Nucl. Mater. 307-311 (2002) 769.
-
3李明,周张健,何培,许迎利,马垚,黎兴刚,燕青芝,葛昌纯.热处理工艺对氧化物弥散强化Fe-Cr合金微观结构和致密化的影响[J].原子能科学技术,2009,43(6):552-555. 被引量:4
-
4A. Alamo, V. Lambard, X. Averty, et al. Assessment of ODS-14%Cr ferritic alloy for high temperature applications [J]. Jour- nal of Nuclear Materials, 329 -330 (2004) 333-337.
-
5R.L. Klueh, J.P. Shingledecker, R. W. Swindeman, et al. Oxide dispersion -- strengthened steels t A comparison of some commercial and experimental alloys[J]. Fusion Eng. Des. 341(2005)103-114.
二级参考文献22
-
1MARIO S, KATSUYA I, HITOSHI S, TADAYUKI F, TADASHI I, OKAMOTO K I. Solar thermal thruster made of single crystal molybdenum [J]. Acta Astronautica,1997, 41 (1): 23-28.
-
2MASAHIRO N, TETSUO Y, JUN T, YUTAKA H. Improvement in recrystallization temperature and mechanical properties of a commercial TZM alloy through microstructure control by multi-step internal nitriding[J]. Materials Transactions JIM, 2005 46(10): 2129-2134.
-
3KUMAR A, EYRE B L. Grain boundary segregation and intergranular fracture in molybdenum[J]. Proc R Soc Lond, 1980, A370:431-458.
-
4MASAHIRO N, YOSHITO T, TETSUO Y, JUN T, YUTAKA H. Preparation of structurally controlled dilute molybdenumtitanium alloys through a novel multi-step internal nitriding technique and their mechanical properties[J]. Mater Sci Eng A,2005, 406(1/2): 50-56.
-
5HIROAKI K, YUJI K, YUTAKA H, TAMAKI S, HIDEO K. Development of molybdenum alloy with high toughness at low temperatures[J]. Materials Transactions JIM, 1996, 37(1): 89-97.
-
6INOUE T, HIRAOKA Y, SUKEDAI E. Hardening behavior of dilute Mo-Ti alloys by two-step heat-treatment[J]. International Journal of Refractory Metals and Hard Materials, 2007, 25: 138-143.
-
7AGNEW S R, LEONHARDT T. The low-temperature mechanical behavior of molybdenum-rhenium[J]. JOM, 2003, 55(10): 25-29.
-
8WADSWORTH J, PACKER C M, CHEWEY P M, COONS W J. A microstructure investigation of the origin of brittle behavior in the transverse direction in Mo-based alloy bars[J]. Metallurgical Transactions A, 1984, 15(9): 1741-1752.
-
9HIRAOKA Y, HIROAKI I, TAKESHI I. Application of fractography to the study of carbon diffusion in molybdenum[J]. Journal of Alloys and Compounds, 2004, 377:127-132.
-
10HIRAOKA Y, KURISHITA H, NARUI M, KAYANO H. Fracture and ductile-to-brittle transition characteristics of molybdenum by impact and static bend tests[J]. Materials Transactions JIM, 1995, 36(4): 504-510.
共引文献14
-
1黄永章,李兴彦,王力军,罗远辉,张力,陈松.高抗拉强度纯钼棒的制备和组织研究[J].稀有金属,2010,34(5):684-688. 被引量:7
-
2赵大鹏,刘咏,刘峰,张刘杰,刘东华,窦玉海.添加球磨粉末对铁基高温合金锻态显微组织与力学性能的影响[J].粉末冶金材料科学与工程,2011,16(4):580-586. 被引量:1
-
3李永志,纪良波,都学飞.纯钼粉末烧结体材料单轴压缩成形的流变应力和致密影响因素[J].热加工工艺,2011,40(20):15-17. 被引量:1
-
4雷玉成,任闻杰,谢伟峰,黄巍.氧化物弥散强化MGH956合金TIG焊缝气孔问题分析[J].焊接学报,2011,32(11):1-4. 被引量:10
-
5李永志,薛克敏,李萍,汪洋,白小波.可压缩纯钼粉末烧结材料的塑性变形行为及影响因素[J].粉末冶金材料科学与工程,2011,16(6):849-855. 被引量:2
-
6廖璐,周张健,李明.14CrODS铁素体钢的制备及其拉伸性能[J].材料工程,2012,40(4):42-46. 被引量:5
-
7李永志,于福义,白小波.纯钼粉末包套等径角挤压致密化行为[J].粉末冶金材料科学与工程,2013,18(4):594-598. 被引量:3
-
8黄江波,魏修宇,李光宗,张外平,夏艳成,常理,宋立强.热轧变形量及退火工艺对钼板材组织和性能的影响[J].硬质合金,2013,30(5):270-274. 被引量:8
-
9龚梦强,周张健,张珂,户赫龙.退火温度与Ti、Al元素对14Cr-ODS合金力学性能的影响[J].粉末冶金材料科学与工程,2015,20(3):356-361. 被引量:4
-
10王峰,张焜,冯娟妮,刘涛.不同规格中频炉对钼制品质量的影响[J].中国钨业,2016,31(2):58-62.
-
1刘强,周海涛,丁洪波,李夏雷,周啸.退火工艺对Mg-8Li-3Al-1Y镁锂合金组织和力学性能的影响[J].热处理技术与装备,2016,37(6):18-23. 被引量:2
-
2杨攀,刘云明,姜强,姚力夫,张毅勇.退火对Zr-4合金复合板组织和性能的影响[J].金属热处理,2016,41(8):72-75. 被引量:2