摘要 催化烟机入口高温烟气管线发生裂纹,在对此类故障的简短回顾之后,采用应力分析软件对此管道做了分析。根据应力计算结果和可能的失效原因,分析得出了审慎的结论以及一些整改建议。 Cracks on the hot flue gas tube to FCC Expander was observed. After a brief review, stress analysis computation for the tube was performed. Failure analysis on all possible reasons with field constraints and computed result leads to a prudent conclusion, with advices of amendment.
作者 戴毅 王佳兵
出处 《广东化工》 CAS 2012年第3期172-175,共4页 Guangdong Chemical Industry
关键词 应力分析 烟气管线 磨蚀:次生相 stress analysis: flue gas tube: erosion: secondary phase
  • 相关文献

参考文献10

  • 1R A White.Material Selection for Petroleum Refineries and Gathering Facilities,NACE International,1998,2,41.
  • 2Liang-Chuan Peng,Tsen-Loong Peng.Pipe Stress Engineering.ASME Press,2009,2:366-368.
  • 3Chevron Corp.Welding Manual,Welding fundamentals,Chevron Corporation,1998:85-100.
  • 4C P Dillon,Material Selection for the Chemical Process Industries,McGraw-Hill,1992,60:305.
  • 5孙秋霞.材料腐蚀与防护,冶金工业出版社,2004,3:70.
  • 6Incoloy?Alloy 800,Data Sheet,Special Metals.
  • 7GB/T983-1995《不锈钢焊条》[S].并参见AWS A5,22-1995(R2005).
  • 8Avesta Welding Manual,pp.16~19,Outokumpu Company,2004.
  • 9ASM Metals Handbook,6:900.
  • 10AWS A5.22-1995(R2005)..,..

同被引文献17

引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部