锌浸渣的浮选高硫产品中硫磺与闪锌矿的分离 被引量:3

Study on Separating Sulfur from Sphalerite in Leached Zinc Residue After Floatation
下载PDF
导出
摘要 针对广东某冶炼厂锌加压浸出渣浮选后的高硫产品,采用抑锌浮硫工艺,以硫化钠和OL-IID为抑制剂、六偏磷酸钠为分散剂进行硫磺与闪锌矿的浮选分离,经1次粗选、2次扫选、4次精浮,最终得到硫品位为92.23%、含锌2.45%的硫磺精矿,以及锌品位为12.97%、含硫73.10%的锌精矿。与现有工艺相比,锌与硫得到了有效的分离与回收。 Based on a kind of high sulphur products pressure-leached from zinc by means of sulphur preferential floatation,with interaction of sodium sulfide and OL-IID, as the depressant, and hexametaphosphate, as the despersing agent, earriedout the floatation separation of sulfur from sphalerite. Through the process of single-stage roughing, two-stage scavenging and four-stage cleaning, and eventually, the sulfur and zinc concentration respectively contain 92. 23% of sulfur with 2.45% of zinc, and 73.10% of sulfur with 12. 97% of zinc ,The Zinc and sulfur get effective separation and recovery compared to current process,
出处 《金属矿山》 CAS 北大核心 2012年第3期149-151,共3页 Metal Mine
基金 教育部高等学校博士点基金项目(编号:20090162110053)
关键词 浸出渣 抑锌浮硫 锌硫分离 Leached residue, Zinc suppression and sulfur floatation, Separation sulfur from zinc
  • 相关文献

参考文献3

二级参考文献4

共引文献30

同被引文献19

引证文献3

二级引证文献6

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部