摘要 Copolymers of methyl methacrylate (MMA) and acrylate terminated poly(ethylene oxide-co-ethylene carbonate) (PEOC) macromonomer (PEOCA) were synthesized, and the degradation of the polymers was investigated by use of quartz crystal microbalance with dissipation (QCM-D). It is shown that the polymeric surface exhibits degradation in seawater depending on the content of the side chains. Field tests in seawater show that the surface constructed by the copolymer can effectively inhibit marine biofouling because it can be self-renewed due to degradation of the copolymer. Copolymers of methyl methacrylate (MMA) and acrylate terminated poly(ethylene oxide-co-ethylene carbonate) (PEOC) macromonomer (PEOCA) were synthesized, and the degradation of the polymers was investigated by use of quartz crystal microbalance with dissipation (QCM-D). It is shown that the polymeric surface exhibits degradation in seawater depending on the content of the side chains. Field tests in seawater show that the surface constructed by the copolymer can effectively inhibit marine biofouling because it can be self-renewed due to degradation of the copolymer.
出处 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2012年第3期337-342,共6页 高分子科学(英文版)
基金 financially supported by the Ministry of Science and Technology of China(No.2012CB933802) the Fundamental Research Funds for Central Universities
关键词 Anti-biofouling DEGRADATION Poly(ethylene carbonate) Poly(ethylene oxide). Anti-biofouling Degradation Poly(ethylene carbonate) Poly(ethylene oxide).
  • 相关文献

参考文献32

  • 1Yebra,D.M.,Kiil,S.and Dam-Johansen,K.,Prog.Org.Coat.,2004,50:75.
  • 2Xie,L.Y.,Hong,F.,Liu,J.H.,Zhang,G.Z.and Wu,C.,Acta Polymerica Sinica(in Chinese),2012,(1):1.
  • 3Callow,J.A.and Callow,M.E.,Nat.Commun.,2011,2:244.
  • 4Finnie,A.and Williams,D.N.,"Paint and coatings technology for the control of marine fouling in biofouling",Wiley-Blackwell, Chichester,U.K.,2010,p.429.
  • 5Thomas,K.V.and Brooks,S.,Biofouling,2010,26:73.
  • 6Beigbeder,A.,Degee,P.,Conlan,S.L.,Mutton,R.J.,Clare,A.S.,Pettitt,M.E.,Callow,M.E.,Callow,J.A.and Dubois,P.,Biofouling,2008,24:291.
  • 7Sommer,S.,Ekin,A.,Webster,D.C.,Stafslien,S.,Daniels,J.,Van Der Wal,L.J.,Thompson,S.E.Y.,Callow,M.E.and Callow,J.A.,Biofouling,2010,26:961.
  • 8Magin,CM.,Long,C.J.,Cooper,S.P.,Ista,L.K.,Lopez,G.P.and Brennan,A.B.,Biofouling,2010,26:719.
  • 9Schumacher,J.F.,Aldred,N.,Callow,M.E.,Finlay,J.A.,Callow,J.A.,Clare,A.S.and Brennan,A.B.,Biofouling, 2007,23:307.
  • 10Schumacher,J.F.,Carman,M.L.,Estes,T.G.,Feinberg,A.W.,Wilson,L.H.,Callow,M.E.,Callow,J.A.,Finlay,J.A.and Brennan,A.B.,Biofouling,2007,23:55.

同被引文献23

  • 1Champ M A. Economic and environmental impacts on ports and harbors from the convention to ban harmful marine anti- fouling systems [ J ]. Marine Pollution Bulletin, 2003,46 (8) :935 -940.
  • 2Tsuji H, Ikarashi K. In vitro hydrolysis of poly ( L- lactide) crystalline residues as extended-chain crystallites III. Effects of pH and enzyme [ J ]. Polymer Degradation and Stability, 2004,85( 1 ) :647 -656.
  • 3Tang R, Palumbo R N, Ji W H, et al. Poly (orthoesteram- ides) : Acid - Labile Temperature - Responsive Copolymers for Potential Biomedical Applications [ J ]. Biomacromolecules, 2009,10(4) :722 -727.
  • 4Tang R, Ji W H, Panus D, et al. Block Copolymer Micelles with Acid - Labile Ortho Ester Side- Chains : Synthesis, Char- acterization, and Enhanced Drug Delivery to Human Glioma Cells[ J]. Journal of Controlled Release, 2011,151 ( 1 ): 18 - 27.
  • 5Zhao Z X, Liu Y, Hu Y F, et al. Enzymatic degradation of block copolymers obtained by sequential ring opening poly- merization of L - lactide and 8 - caprolactone [ J ]. Polymer Degradation and Stability ,2007,92 ( 10 ) : 1 769 - 1 777.
  • 6Antheunis H, Meer J V, Geus M D, et al. Autocatalytic Equation Describing the Change in Molecular Weight during Hydrolytic Degradation of Aliphatic Polyesters [ J ]. Biomac- romolecules,2010,11 (4) : 1 118 - 1 124.
  • 7Liu F, Zhao Z X, Yang J, et al. Enzyme - catalyzed degrada- tion of poly ( L - laetide )/poly ( - - caprolactone ) diblock, triblock and four- armed copolymers [ J ]. Polymer Degrada- tion and Stability,2009,94 (2) :227 - 233.
  • 8Ma C F,Hou Y,Liu S,et al. Effect of Microphase Separation on the Protein Resistance of a Polymeric Surface[J]. Lang- muir,2009,25 (16) :9 467 - 9 472.
  • 9Ma C F, Xu L G, Xu W T, et al. Degradable polyurethane for marine anti-biofouling[ J ]. Journal of Materials Chemis- try B,2013,24(1) :3 099 -3 106.
  • 10Bodkhe R B,Thompson S E M, Yehle C, et al. The effect of formulation variables on fouling-release performance of strat- ified siloxane- polyurethane coatings [ J ]. Journal of Coatings Technology and Research,2012,9 (3) :235 - 249.

引证文献2

二级引证文献8

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部