摘要
采用真空热爆加压法 (简称VTEP)工艺制备了高粒子含量TiCp/ 2 0 2 4复合材料。通过数据采集器记录了不同铝含量时热爆反应的时间—温度曲线 ;通过XRD分析了TiCp/ 2 0 2 4复合材料的相组成 ;用SEM和TEM观察了TiCp/ 2 0 2 4复合材料的显微组织、微观结构和断口形貌。结果表明 :VTEP工艺可以获得颗粒细小圆整、分布均匀、致密的高颗粒含量TiCp/ 2 0 2 4复合材料。
The TiC p/2024 Composites with high particles content were prepared by vacuum thermal explosion and pressure process(VTEP). The curves of temperature vs time were recorded by data collection instrument. The phase composition of the TiC p/2024 composites was analyzed by XRD method, and the fracture morphology and microstructure of TiC p/2024 composites were observed by SEM and TEM. The result showed that the dense TiC p/2024 composites with high particles content , fine grained and uniform distribution can be obtained by VTEP.
出处
《宇航材料工艺》
CAS
CSCD
北大核心
2000年第1期59-63,共5页
Aerospace Materials & Technology
基金
先进复合材料国防科技重点实验室基金资助项目 !编号 97JS49.4/HT0 10 8
关键词
真空热爆加压法
TiCp/2024复合材料
VTEP
Vacuum thermal explosion pressures,TiC p/2024 composites,Phase composition, Microstructure, Fracture morphology