采用钨极氩弧焊方法对准0.7 mm的65Mn钢丝进行了焊接试验研究,获得了最佳焊接电流及热处理工艺参数,达到了强度、弹性及抗疲劳性能的要求。
The welding test of 65Mn steel wire(φ0.7 mm)was carried out by Argo tungsten-arc welding.The optimal welding current and process parameters of heat treatment were obtained,and the requirements of strength,elasticity and anti-fatigue were achieved.