摘要
分析了选矿厂矿石性质和细泥尾矿综合回收工艺,对细泥尾矿综合回收工艺进行改造。工艺改造后铋回收率提高了25.07%,可多回收铋金属6.250 1 t/a;钨回收率提高了10.13%,可多回收钨精矿2.639 1 t/a。
The comprehensive recovery technology of a fine mud tailing is upgraded based on analyzing the ore properties and the former recovery technology. The recovery rates of bismuth and tungsten increase by 25.07 % and 10.13 % with additional bismuth and tungsten amounted to 6.250 1 t/a and 2.639 1 t/a respectively.
出处
《中国钨业》
CAS
2012年第2期19-21,共3页
China Tungsten Industry
关键词
工艺改进
综合回收
铋金属
钨精矿
回收率
technology upgrade
comprehensive recovery
bismuth
tungsten concentrate
recovery rate