摘要
简要介绍了华北某贫赤褐铁矿的矿石性质,重点研究了磨矿产品细度和反浮选药剂用量对产品指标的影响。试验研究结果表明,采用2阶段磨矿,1次中磁1次强磁预先抛废,1粗1精3扫、中矿顺序返回闭路反浮选流程处理,可以获得铁品位为66.07%、铁回收率为80.53%的精矿。
Briefly introduced the ore properties of a lean hematite-limonite ore in North China. The influence of particle size of the grinding product and reagent dosage to flotation index were mainly studied. A reverse flotation closed circuit consisting of two-staged grinding, one middle-density magnetic and one high-density magnetic seperation to discard tailings, one roughing, one cleaning and three scavengings, separation middlings order to return could get the iron grade of 66.07% and iron recovery of 80. 53%.
出处
《金属矿山》
CAS
北大核心
2012年第5期82-84,共3页
Metal Mine
关键词
赤褐铁矿
磁选
阴离子反浮选
Hematite-limonite ore, Magnetic separation, Anionic reverse flotation