期刊文献+

含碳球团的还原性和还原冷却后的强度 被引量:10

Reduction and Strength after Reduction of Cooled Pellet Contain Carbon
下载PDF
导出
摘要 在 1273~1573 K条件下研究了不同煤种、木炭和石墨与不同种类矿石制成含碳球团 的还原速度;进而讨论了温度、配碳比(C/O)、挥发分含量等因素对含碳球团还原所需时间和 金属化率的影响.通过测定含碳球团还原冷却后的强度,对影响强度因素进行了分析.还原冷 却后的强度在温度 1273 K时较低,配入含挥发分较高的气煤,可以使还原冷却后的强度提高, 加快反应速度. The reduction experiment of the pellets containing carbon, which consist of different kinds of iron ore and coal (including graphite and charcoal), was carbon out. The effect of temperature, rate of carbon and volatility etc. on the reduction time and metallization of the pellets has been discussed. The strength of the reduced and cooled pellets was measured and the influence of the factors was analysed. The strength of pellets at temperature 1 273 K is low. When the gas coal of high volatility is added, the pellet is becoming to be reduced quickly and its strength is increased.
出处 《北京科技大学学报》 EI CAS CSCD 北大核心 2000年第2期101-104,共4页 Journal of University of Science and Technology Beijing
基金 国家"攀登计划"重点项目
关键词 含碳球团 还原后强度 团矿 高温还原 还原性 pellet containing carbon strength after being reduced and cooled reduction at high temperature smelting reduction
  • 相关文献

参考文献5

  • 1煤炭科学院煤化所.煤质与炼焦[M].北京:煤炭工业出版社,1985..
  • 2杜挺,钢铁冶炼新工艺,1994年
  • 3Bryk C,Ironmaking Steelmaking,1986年,13卷,2期,70页
  • 4煤炭科学院煤化所,煤质与炼焦,1985年
  • 5李海珠,铁と钢,1971年,57卷,3期,465页

同被引文献62

引证文献10

二级引证文献31

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部