摘要
以NiCl2为原料,CO(NH2)2为沉淀剂,采用均匀沉淀法,制备了纳米氧化镍粒子.在制备过程中添加适量的NP-10及适量有机溶剂作为分散剂.采用透射电镜、X-射线衍射仪、热重-差热分析仪对粒子的化学组成及性能进行了表征.
Nanometer-sized NiO particles were prepared by chemical sedimentation method with NiCl2 as raw material and CO (NH2 )2 as precipitant. Appropriate amount of NP-10 and organic added to the Nano-oxidation of nickel particles in preparation process. The chemical of the particles were characterized by TG-DTA,XRD,TEM.
出处
《吉林化工学院学报》
CAS
2012年第5期8-10,共3页
Journal of Jilin Institute of Chemical Technology
基金
吉林化工学院分析测试基金项目(2011103006)
关键词
纳米
氧化镍
化学沉淀法
nanometer
nickel oxide
chemical sedimentation method solvents as dispersant was composition and properties