摘要 采用热重红外联用分析和热解气质联用分析技术,考察了红橡木材包装废弃物的热分解、气相组分生成及分布规律。研究表明:在800℃终温和10℃/min的升温速率条件下,红橡木材包装废弃物的主要热解阶段集中在220~385℃,失重率为78.99%;高温区热解活化能明显低于低温区,说明随着温度的升高较容易发生热解反应;热解初期主要是水分和部分酸类、醛类物质的析出,主要热解阶段为H2O,CO2,CO,CH4和酸类、醛类、酯类等的大量析出,在热解后期主要为CO2和CH4的析出;热解析出的气体主要为含氧官能团的有机化合物,包括酸类(19.29%)、醛类(15.14%)、酯类(9.97%)、酮类(9.00%)、糖类(8.59%)、酚类(5.29%)、醇类(3.63%)等。 Characteristics of thermal decomposition and gas components generation and distribution of wood packaging waste of red oak were investigated using TG-FTIR and Py-GC/MS. The result showed that at 800 ℃ and 10 ℃/rain, the main stage of pyrolysis concentrates in the range of 220-385℃C and the total weight loss is 78.99%; activation energy in high temperature range is significantly lower than that in low temperature range, so it is easier for the thermal decomposition in higher temperature; H20 and part of acids and aldehydes are generated in the initial stage of pyrolysis; A large amount of H2O, CO2, CO, CH4 , acids, aldehydes, esters is released in the main stage; CO2 and CH4 are released in the later stage; the pyrolysis vapors include oxygen- containing functional compounds, such as acids (19.29%), aldehydes (15. 14%), esters (9. 97%), ketones (9.00%) , sugars (8.59%), phenols (5.29%), and alcohols (3. 630%), etc.
机构地区 北京林业大学
出处 《包装工程》 CAS CSCD 北大核心 2012年第13期40-44,共5页 Packaging Engineering
基金 国家自然科学基金资助项目(30972309) 国家教育部博士点基金资助项目(20090014110015) 科技部农业科技成果转化资金资助项目(2010GB23600654)
关键词 木质包装废弃物 红橡木材 热化学特性 热重红外联用 热解气质联用 wood packaging waste red oak thermochemical characteristics TG-FTIR Py-GC/MS
  • 相关文献

参考文献8

二级参考文献48

共引文献119

同被引文献12

引证文献1

二级引证文献7

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部