不同试剂处理对杉木疏水性能的影响 被引量:1

Hydrophobic Property of Chinese Fir Treated with Different Chemicals
下载PDF
导出
摘要 为改善木材的尺寸稳定性,采用二甲基二氯硅烷和聚硅氧烷分别对杉木进行改性处理,并测定处理材的疏水性能。结果表明,处理杉木的平衡含水率下降,杉木质量、与水的接触角和抗膨胀系数等均显著增加。 In order to improve the dimensional stability of Chinese fir, the authors used two formulae of dimethyldichlorosilane and polydimethylsiloxane solutions with n-hexane as the main solvent to treat the wood. The results indicated that the equilibrium moisture content of both treated samples decreased considerably. Surface water contact angle and antiswelling efficiency of treated samples increased.
出处 《木材工业》 北大核心 2012年第4期16-20,共5页 China Wood Industry
基金 林业公益性行业科研专项(201004038)
关键词 杉木 改性 二氯二甲基硅烷 聚硅氧烷 疏水性 Chinese fir modification dimethyldichlorosilane polydimethylsiloxane hydrophobicity
  • 相关文献

参考文献17

  • 1Rowell R M. Chemical modification of wood [J]. Forest Products Abstracts, 1983, 6(12) : 363-382.
  • 2Rowell R M. Chemical modification of wood[M]. Handbook of Wood Chemistry and Wood Composites, 2005 : 381-420.
  • 3Rowell R M. Chemical modification of wood: A short review [J]. Wood Material Science and Engineering, 2006(1):29 -33.
  • 4Ozmen N,Cetin N S. The effect of chemical modification on the strength of wood and bonded wood joints[J]. European Polymer Journal, 2002, 38(7) : 1483-1486.
  • 5Makoto O. FTIR PAS study of light-induced changes in the surface of acetylated or polyethylene glycol-impregnated wood [J]. Journal of Wood Science, 2002, 48(5) :394-401.
  • 6Schneider M H, Phillips J G. Waterborne furfural-urea modification of wood[P]. US Patent: US 2009/0004395 A1, 2009.
  • 7Schneider M H,Phillips J G. High weight percent gain (WPG) furfural-urea modification of wood[P]. US Patent: US 2009/ 0004495 A1, 2009.
  • 8Sakai K,Matsunaga M,Minato K,et al. Effects of impregnation of simple phenolic and natural polycyclic compounds on physical properties of wood[J]. Journal of Wood Science, 1999, 45(3): 227-232.
  • 9Deka M, Saikia C N. Chemical modification of wood with thermosetting resin: effect on dimensional stability and strength property[J]. Bioresource Technology, 2000, 73(2) : 179-181.
  • 10Donath S, Militz H, Mai C. Wood modification with alkoxysilanes[J]. Wood Science and Technology, 2004, 38 (7) :555-566.

二级参考文献1

  • 1刘正添,实木化学,1988年

共引文献8

同被引文献11

  • 1Mohebby B,GorbaniKokandeh M, Soltani M.Springback in acetylated wood based composites[J]. Construction and Building Materials,2009,23(9):3103-3106.
  • 2Li J Z, Furuno T, Zhou W R,et al. Properties of acetylated wood prepared at low temperature in the presence of catalysts[J]. Journal of Wood Chemistry and Technology,2009,29(3):241-250.
  • 3Gindl W , Schberl T. The significance of the elastic modulus of wood cell walls obtained from nanoindentation measurements[J]. Composites Part A: Applied Science and Manufacturing,2004,35(11):1345-1349.
  • 4Gindl W, Gupta H S, Grünwald C. Lignification of spruce tracheid secondary cell walls related to longitudinal hardness and modulus of elasticity using nanoindentation[J]. Canadian Journal of Botany,2002,80(10):1029-1033.
  • 5Wang T, Chang L, Yang S,et al. Hydrophobic properties of biomorphic carbon surfaces prepared by sintering lotus leaves[J]. Ceramics International,2013,39(7);8165-8172.
  • 6Adusumalli R B, Mook W M, Passas R,et al. Nanoindentation of single pulp fibre cell walls[J]. Journal of Materials Science,2010,45(10):2558-2563.
  • 7Lee S H, Wang S, Pharr G M,et al. Mechanical properties and creep behavior of lyocell fibers by nanoindentation and nanotensile testing[J]. Holzforschung,2007,61(3):254-260.
  • 8王金霞,刘温霞.AKD施胶机理综述[J].纸和造纸,2011,30(3):47-50. 被引量:17
  • 9杨蕊,周定国,王思群,张洋,吴燕.木质材料表面疏水性能的研究进展[J].木材工业,2012,26(6):26-29. 被引量:4
  • 10林浩,樊玉平,田又新.浸渍增重率和反渗率研究[J].炭素技术,2003,22(4):20-24. 被引量:3

引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部