热压膜材料力学性能恒温水浴测试系统的建立
摘要
热压膜材料在口腔医学领域应用广泛,可用于制作保持器、牙周夹板、磨牙垫和颌间固定装置等。
出处
《中华口腔医学杂志》
CAS
CSCD
北大核心
2012年第8期505-506,共2页
Chinese Journal of Stomatology
基金
国家自然科学基金(30872914)
参考文献14
-
1白玉兴,王邦康.无托槽隐形矫治技术——口腔正畸的机遇与挑战[J].华西口腔医学杂志,2007,25(6):521-524. 被引量:46
-
2Lloyd T, Nightingale C, Edler R. The use of vacuum-formed splints for temporary intermaxillary fixation in the management of unilateral condylar fractures. Br J Oral Maxillofac Surg, 2001, 39(4) : 301-303.
-
3Oh WS, Wang C. Use of thermoplastic vacuum-formed matrix for emergency management of crown-root fracture. J Prosthet Dent, 2007, 98(4) : 335-336.
-
4Tuncay OC. The Invisalign System. Philadelphia: Quintessence, 2006: 3-10,177-186.
-
5法晨,潘晓岗,田杰.无托槽隐形矫治器的临床研究进展[J].口腔材料器械杂志,2010,19(1):30-33. 被引量:17
-
6Kwon JS, Lee YK, Lim BS, et al. Force delivery properties of thermoplastic orthodontic materials. Am J Orthod Dentofacial Orthop, 2008, 133(2) : 228-234.
-
7Ryokawa H, Miyazaki Y, Fujishima A, et al. The mechanical properties of dental thermoplastic materials in a simulated intraoral environment. Orthodontic Waves, 2006,65 (6) :64-72.
-
8张宁,白玉兴,张昆亚,任超超,周洁珉,祁鹏.不同厚度热压膜材料的力学性能研究[J].北京口腔医学,2009,17(4):184-186. 被引量:20
-
9张宁,方东煜,白玉兴,丁雪佳,张雨.四种热压膜正畸材料力学性能的比较[J].中华口腔医学杂志,2011,46(9):551-553. 被引量:8
-
10国家质检总局.GB/T1040.34006塑料拉伸性能的测定第3部分:薄膜和薄片的试验条件.北京:中国标准出版社,2006.
二级参考文献64
-
1王邦康.口腔正畸矫治方法的新进展——无托槽隐形矫治器的研究与展望[J].北京口腔医学,2005,13(1):2-5. 被引量:27
-
2周洁珉,白玉兴,王邦康.数字化三维牙颌模型测量系统的可靠性对比研究[J].现代口腔医学杂志,2005,19(4):367-368. 被引量:18
-
3田杰,郑云天,周凯,潘裕炯.无托槽隐形矫治技术矫治牙列间隙1例报道[J].实用口腔医学杂志,2007,23(2):302-303. 被引量:7
-
4Boyd RL, Miller R J, Vlaskalic V. The Invisalign System in adult orthodontics: mild crowding and space closure cases. J Clin Orthod 2000,34(4) :203-212.
-
5Wong BH. Invisalign A to Z. Am J Orthod Dentofacial Orthop,2002, 121 (5) :521-524.
-
6Kuo E, Miller RJ. Automated custom-manufacturing technology in orthodontics. Am J Orthod Dentofacial Orthop,2003,123 (5):578- 581.
-
7Vlakalic V, Boyd RL. Clinical evolution of the Invisalign appliance. J Calif Dent Assoc,2002,30 (10) :769-776.
-
8Bollen AM, Huang G, King G, et al. Activation time and material stiffness of sequential removable orthodontic appliances. Part 1: Ability to complete treatment. Am J Orthod Dentofacial Orthop,2003, 124 ( 5 ) :496-501.
-
9Clements KM, Bollen AM, Huang G, et al. Activation time and material stiffness of sequential removable orthodontic appliances. Part 2 :Dental improvements. Am J Orthod Dentofacial Orthop, 2003,124 (5) :502-508.
-
10GD Gardner, Dunn WJ, Taloumis L. Wear comparison of thermoplastic materials used for orthodontic retainers. Am J Orthod Dentofacial Orthop,2003,124 (3) :294-297.
共引文献77
-
1徐琦,张晓蓉.隐形矫治技术的发展和临床应用[J].昆明医科大学学报,2012,33(S1):116-119. 被引量:1
-
2李丽岩.隐形矫治技术矫治成人严重拥挤后复发一例[J].中国美容医学,2008,17(12):1783-1784. 被引量:1
-
3白玉兴,杨斌,戴青,田杰,祁鹏,王邦康.牙周病致前牙间隙患者的无托槽隐形矫治初探[J].中华口腔医学杂志,2009,44(7):421-424. 被引量:7
-
4张宁,白玉兴,张昆亚,任超超,周洁珉,祁鹏.不同厚度热压膜材料的力学性能研究[J].北京口腔医学,2009,17(4):184-186. 被引量:20
-
5张云飞,金钫,刘鑫,刘震寰,刘岗.三维数字化正畸软件OrthoRx的研发及其临床应用[J].实用口腔医学杂志,2009,25(5):672-676. 被引量:5
-
6张宁,白玉兴.热压膜材料的研究及临床应用进展[J].北京口腔医学,2009,17(6):354-356. 被引量:9
-
7张宁,白玉兴,张昆亚,任超超,周洁珉,祁鹏.不同厚度热压膜材料厚度稳定性的研究[J].华西口腔医学杂志,2010,28(1):99-101. 被引量:13
-
8张宁,白玉兴,张昆亚.正畸用热压膜材料的力学性能分析[J].中华医学杂志,2010,90(34):2412-2414. 被引量:4
-
9马亚奇,李忠科,王先泽.基于测地路径的牙齿模型交互分割算法研究[J].中国图象图形学报,2011,16(4):554-558. 被引量:5
-
10侯伟,陈彬,穆超,陈文静.无托槽隐形矫治技术矫治牙列拥挤的临床研究[J].南京医科大学学报(自然科学版),2011,31(9):1364-1368. 被引量:12
-
1王振军,侯书健,史芸,张元信,程国良.手部严重热压伤20例的临床治疗[J].青岛医药卫生,2002,34(1):6-7.
-
2罗培寿.热压油烧伤并重度吸入性损伤的护理[J].护士进修杂志,1996,11(1):39-39.
-
3张涛,唐公杰,王新波.热压伤34例治疗体会[J].实用临床医学(江西),2003,4(3):50-50. 被引量:1
-
4薄存朋,于庆平.热压伤34例治疗体会[J].社区医学杂志,2004,2(2):80-81.
-
5李旭奎.个体化牙周夹板在治疗儿童下颌骨骨折中的应用[J].基层医学论坛,2009,13(10):307-308. 被引量:2
-
6张宁,白玉兴.热压膜材料的研究及临床应用进展[J].北京口腔医学,2009,17(6):354-356. 被引量:9
-
7林谋俊.烧伤休克期应用恒温水浴加温补液法治疗38例临床观察[J].中国民族民间医药,2014,23(24):59-59.
-
8应锡钧,史振军,穆雄铮.手部热压伤的创面修复(附30例分析)[J].中国医师杂志,2002,4(11):1262-1263.
-
9祁俊,吴杨炀,胡克苏,张逸,张云.Wnt5a在严重烫伤大鼠早期肠黏膜组织中的表达及意义[J].武汉大学学报(医学版),2013,34(5):699-702.
-
10王新,朱权,严瑾,张萍,杨威,肖年来,熊卜贵.热压伤的临床治疗分析[J].中国医药,2010,5(6):543-544. 被引量:1