球磨时间对固相法制备ZrW_2O_8的影响

Effect of Ball Milling Time on Synthesis of ZrW_2O_8 through Solid Reaction Method
下载PDF
导出
摘要 目前,ZrW_2O_8的制备方法主要有固相反应法和湿化学法。以ZrO_2和WO_3为原料,采用固相法制备了ZrW2O_8。结果表明,ZrW_2O_8的含量随球磨时间的增加而减小,且球磨时间越长,烧结样品中越容易出现γ-ZrW_2O_8(正交相)。 At present, ZrW2O8 is generally synthesized by solid reaction method or wei-chemical process. ZrW20s has been synthesized through solid reaction method using ZrO2 and WO3 as the raw materials. The results reveal that as the ball milling time increases, the ZrW2O8 content reduces , and γ-ZrW2O8 is easier to obtain in the sintered sample.
出处 《热处理》 CAS 2012年第4期20-22,共3页 Heat Treatment
关键词 固相反应法 球磨时间 钨酸锆 solid reaction method ball milling time zirconium tungstate
  • 相关文献

参考文献8

  • 1Evans J S O, Mary T A, Vogt T, et al. Negative thermal expansion in ZrW208 and HfW208 [J]. Chemistry of Materials, 1996, 8 (12) : 2809-2823.
  • 2Mary T A, Evans J S O, Vogt T, et al. Negative thermal expansion from 0.3 to 1050 Kelvin in ZrW208 [J]. Science, 1996, 272(5258): 90-92.
  • 3Evans J S O, David W I F, Sleigh! A W. Structural investigation of the negative-thermal-expansion material ZrW208 [ J ]. Acta Crystal, 1999, B55: 333-340.
  • 4Yamamura Y, Nakajima N, Tsuji T. Heat capacity anormaly due to the α to β structural phase transition in ZrW208 [ J ]. Solid State Communications, 2000 (114) : 453-455.
  • 5程晓农,孙秀娟,杨娟,徐桂芳.固相法合成负热膨胀性粉体ZrW_2O_8[J].江苏大学学报(自然科学版),2005,26(4):350-353. 被引量:30
  • 6邢奇凤,邢献然,杜凌,于然波,陈骏,邓金侠,罗君.水热法合成负热膨胀材料ZrW_2O_8[J].金属学报,2005,41(6):669-672. 被引量:14
  • 7杜学丽,曲选辉,秦明礼,郭瑞松.共沉淀法制备负膨胀系数材料ZrW_2O_8[J].北京科技大学学报,2007,29(9):925-927. 被引量:6
  • 8Kameswari U, Sleight A W, Evans J S 0. Rapid synthesis of ZrW208 and related phases and Structure refinement of ZrWMoO8[J]. Int. J. Inorganic Materials, 2000, 2: 333-337.

二级参考文献36

  • 1韩海滨,张可成,李金平.ZrW_2O_8负膨胀陶瓷材料进展[J].硅酸盐通报,2005,24(1):85-88. 被引量:7
  • 2邢奇凤,邢献然,杜凌,于然波,陈骏,邓金侠,罗君.水热法合成负热膨胀材料ZrW_2O_8[J].金属学报,2005,41(6):669-672. 被引量:14
  • 3程晓农,孙秀娟,杨娟,徐桂芳.固相法合成负热膨胀性粉体ZrW_2O_8[J].江苏大学学报(自然科学版),2005,26(4):350-353. 被引量:30
  • 4孙秀娟,杨娟,刘芹芹,程晓农.共沉淀法制备负热膨胀性ZrW_2O_8粉体及其粒径控制初探[J].无机化学学报,2005,21(9):1412-1416. 被引量:11
  • 5Mary T A, Evans J S O, Vogt T, Sleight A W. Negative thermal expansion from 0. 3 to 1 050 Kelvin in ZrW2O8[J]. Science, 1996,272:90 -92.
  • 6Evans J S O, Mary T A, Vogt T, Subramanian M A,Sleight A W. Negative thermal expansion in ZrW2O8 and HfW2O8 [ J]. Chem Mater, 1996(8) :2809 - 2823.
  • 7Kameswari U, Sleight A W,Evans J S O. Rapid synthesis of ZrW2O8 and related phase and structure refinement of ZrWMoO8 [ J ]. Inter J of Inorg Mater, 2000 ( 2 ): 333 -337.
  • 8Sleight A W. Compounds that contract on heating[ J]. Inorg Chem, 1998,37:2854 - 2860.
  • 9Sleight A W. Negative thermal expansion materials [J].Synthesis and Reactivity of Solids, 1998(3) :128 -131.
  • 10MORITO Yuko, WANG Shaorong, OHSHIMA Yoshikazu. Preparation of dense negative thermal expansion oxide by rapid quenching of ZrW2O8 melt [ J ]. J Ceram Soc Japan,2002 (6): 544 - 548.

共引文献38

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部