摘要 目的:评价侧向加载条件下纤维桩在根管内的长度对纤维桩复合树脂核修复体抗折性能的影响。方法:选择下颌单根管前磨牙36颗,随机分为6mm、9mm和12mm的3个组,将离体牙行纤维桩修复后使用速率为0.2mm/min的135°角侧向加载。结果:桩长度为6mm组的荷载力值明显的低于其余2组的荷载力值,其差异有统计学意义(P<0.05)。结论:对于纤维桩复合树脂核修复体,当桩在根管内的长度小于临床牙冠时,修复体的抗折能力较低,因此,临床上尽可能的达到一定的长度,以消除临床失败几率。 Objective: To evaluate,the influence of different post lengths upon root fracture resistance. Methods: Thirty six recently extracted single rooted lower premolars from orthodontic patients were divided into 3 groups (6mm,9mm,12mm), 12 teeth each. The specimens were tested in a universal test machine and all samples were loaded until failure. Results: Posts shorter than clinical crown length, demonstrated root fracture under significantly lower loading forces(P〈0.05). Conclusion: Usage of posts shorter than clinical crowns should be avoided to eliminate clinical failure.
出处 《口腔医学研究》 CAS CSCD 2012年第9期907-910,共4页 Journal of Oral Science Research
关键词 桩的长度 玻璃纤维桩 抗折强度 Post length Glass fiber post Fracture resistance
  • 相关文献

参考文献23

二级参考文献26

  • 1李伟,陈吉华,郑亚萍,王辉,王迎捷.新型齿科纤维/树脂桩钉的应用设计及性能研究[J].口腔医学研究,2004,20(6):623-625. 被引量:6
  • 2张翼.柱状阶梯形和螺纹形核桩钉系列的研制及实验研究:[学位论文].西安:第四军医大学,1999..
  • 3Hedlund SO,Johansson NG,Sjogren G.Plasma treatment increased shear bond strength between heat cured acrylic resin and self-curing acrylic resin [J].J Oral Rehabil,2003,30(10):1036-1040.
  • 4Sharaf AA.The application of fiber core posts in restoring badly destroyed primary incisors [J].J Clin Pediatr Dent,2002,26 (3): 217-224.
  • 5Ferrari M,Vichi A,Mannocci F,et al.Retrospective study of the clinical performance of fiber posts [J].Am J Dent,2000,13:9B- 13B.
  • 6Akkayan B,Gulmez T.Resistance to fracture of endodontically treated teeth restored with different post systems [J].J Prosthet Dent,2002,87 (4):431-437.
  • 7Koutayas SO,Kern M.All-ceramic post and core:The state of the art[J].Quintessence Int,1999,30(6):383-392.
  • 8Butz,Heydecke G,Strub JR.Survival rate and fracturestrength of endodontically treated maxillary incisors with moderate defects restored with different post-and-core systems[J].An in virro study.Int J Prosthodont,2001,14:58-64.
  • 9Monticelli F,Goracci C,Ferrai M.Micromorpholopy of the fiber postresin core unit:A scanning electron microscopy evaluation[J].Dent mater,2004,20(2):176-183.
  • 10Andreasen FM, Steinhardt U, Bile M, et al. Bonding of enamel-dentin. Crown fragments after crown fracture,An experimental study using bonding agents [J]. Endod Dent Trau matol, 1993, 9(3) : 111-114.

共引文献49

同被引文献75

引证文献7

二级引证文献17

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部