废旧砖在GRC中的再生利用研究 被引量:7

Research on recycling use of waste brick in GRC
下载PDF
导出
摘要 采用正交设计方法研究了粉煤灰及再生砖骨料对GRC的影响,并进一步研究了再生砖骨料的取代率对再生骨料GRC的影响及变化规律。结果表明,再生骨料GRC的强度随废砖取代率的提高呈增长趋势,当粉煤灰取代普通水泥20%,耐碱玻纤体积率1.5%,废旧砖取代天然砂35%~45%时,可达到或超过天然砂GRC的力学性能;其中再生骨料取代天然砂体积率为45%时,再生骨料GRC的抗折和抗压强度最大,7 d与28 d抗折强度分别可增长38.5%和38.3%,抗压强度分别可增长25.3%和9.1%。 In the paper, by using the orthogonal design method,the effects of fly ash and waste brick aggregate on GRC was researched,the effects of replacement ratio of waste brick aggregate on the recycled aggregate GRC was further researched. The re- suits show that the strength of recycled aggregate GRC improves with the increase of the replacement ratio of waste brick aggre- gate. When the replacement ratio of fly ash to P·O cement was 20%,alkali-resistant glass fiber volume ratio was 1.5% and waste brick to natural sand was 35%-45%,the mechanical properties can reach or exceed to the one of GRC with natural sand;and when the volume replacement ratio reached to 45%,the performance of GRC is optimal, the 7 d and 28 d tensile strength can in- crease 38.5% and 35.3% respectively and the compressive strength can increase 25.3% and 9.1% respectively.
作者 程海丽
出处 《新型建筑材料》 2012年第10期8-10,共3页 New Building Materials
基金 北京市教委科技发展计划项目(KM201210009010)
关键词 GRC 废旧砖 再生骨料 GRC waste brick:recycled aggregate
  • 相关文献

参考文献2

二级参考文献6

  • 1楼宗汉,韩韧,胡国君,盛其仲.关于玻纤水泥碱度问题的研究[J].硅酸盐学报,1996,24(6):609-615. 被引量:11
  • 2张亚梅,学位论文,1998年
  • 3沈荣熹,论改善玻璃纤维增强水泥的长期耐久性的技术途径,1995年
  • 4顾惕人(译),表面的物理化学,1984年
  • 5曹永康,混凝土与水泥制品1997年学术年会论文集,277页
  • 6陈尚,中国硅酸盐学会房建材料专业委员会第四届年会论文集.9,53页

共引文献10

同被引文献41

引证文献7

二级引证文献36

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部