摘要 Reinforcement of TPNR (thermoplastic natural rubber) with cotton fibre spun was prepared by using hot compression moulding. The TPNR was prepared by mixing NR (natural rubber) with PE (polyethylene) using 2-roll mills before compressed on cotton fibre spun and vulcanized at 150℃. The mechanical properties and morphology of the membrane were investigated using DMTA (dynamic mechanical thermal analyzer) and SEM (scanning electron microscopy), respectively. The membrane strength was increased from 10 MPa to 18 MPa after reinforced with cotton fibre spun as well as the increasing of dielectric constant. The membrane was immersed in xylene to remove PE phase before characterization of membrane properties.
出处 《Journal of Chemistry and Chemical Engineering》 2012年第9期799-802,共4页 化学与化工(英文版)
关键词 TPNR natural rubber cotton fibre spun REINFORCEMENT PE. 棉纤维 膜强度 热塑性天然橡胶 扫描电子显微镜 热机械分析仪 纤维纺丝 DMTA 力学性能
  • 相关文献

参考文献9

  • 1Sirisinha, C.; Baulek-Limcharoen, S.; Thunyarittikorn, J. Relationships among Blending Conditions, Size of Dispersed Phase, and Oil Resistance in Natural Rubber and Nitrile Rubber Blends. J. Appl. Polym. Sci. 2001, 82(5), 1232-1237.
  • 2Suksawad, P.; Kosugi, K.; Yamamoto, Y.; Akabori, K.; Kuroda, H.; Kawahara, S. Polymer Electrolyte Membrane with Nanomatrix Channel Prepared by Sulfonation of Natural Rubber Grafted with Polystyrene. Appl. Polym. Sci. 2011, 122(4), 2403-2414.
  • 3Azura, A. R.; Ghazali, S.; Mariatti, M. Effects of the Filler Loading and Aging Time on the Mechanical and Electrical Conductivity Properties of Carbon Black Filled Natural Rubber. J. Appl. Polym. Sci. 2008, 110(2), 747-752.
  • 4Tian, H.; Tian, M.; Zou, H.; Dang, Z.; Zhang, L. Special Electrical Conductivity of Carbon Black-Filled Two-Phased Thermoplastic Vulcanizates. J. Appl. Polym. Sci. 2010, 117(2), 691-699.
  • 5Chang, W.; Ma, G.; Yang, D.; Su, D.; Song, G.; Nie, J. Electrospun Ultrafine Composite Fibers from Organic-Soluble Chitosan and Poly(Ethylene Oxide). J. Appl. Polvm. Sci. 2010, 117(4), 2113-2120.
  • 6Saad, A. L. G.; Younan, A. F. Rheological, Mechanical and Electrical Properties of Natural Rubber-White Filler Mixtures Reinforced with Nylon 6 Short Fibers. Polymer Degradation and Stability 1995, 50(2), 133-140.
  • 7Ortiz-Serna, P.; Diaz-Calleja, R.; Sanchis, M. J.; Riande, E.; Nunes, R.; Martins, A.; et al. Dielectric Spectroscopy of Natural Rubber-Cellulose II Nanocomposites. Journal of Non-Crystalline Solids 2011, 357(2), 598-604.
  • 8Johns, J.; Nakason, C. Dielectric Properties of Natural Rubber/Chitosan Blends: Effects of Blend Ratio and Compatibilization. Journal of Non-Crystalline Solids 2011, 357(1), 1816-1821.
  • 9Lewis, C. K.; Misaen, B.; Changchum, S. Effect of Process and Formulation Variables on Properties of Extrude EPDM Foam. Songklanakarin J. Sci. Technol. 1999, 21(3), 16-25.

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部