摘要
介绍了108 m3聚合釜热水入料的改造方案,改造后生产周期缩短了80~90 min,有效提高了PVC产量。
Renovation plan of hot water feeding for 108 m3 polymerizer was introduced.After renovation,the production period could be shortened by 80-90 minutes,and thus the output of PVC could be increased effectively.
出处
《聚氯乙烯》
CAS
2012年第10期13-15,共3页
Polyvinyl Chloride
关键词
PVC
聚合釜
热水入料
扩能
改造
PVC
polymerizer
hot water feeding
capacity expansion
renovation