锻造掺杂La_2O_3合金钼棒退火过程的组织演变和再结晶动力学 被引量:2

MICROSTRUCTURE EVOLUTION AND STATIC RECRYSTALLIZATION KINETICS OF FORGING La_2O_3-DOPED Mo ALLOY
下载PDF
导出
摘要 对锻造掺杂La2O3合金钼棒在1 360~1 500℃之间的静态再结晶组织演变和动力学机制进行了研究。结果表明,再结晶分数与退火时间之间的关系可以用J-M方程来描述。根据动力学分析,可以计算出掺杂La2O3合金钼棒的再结晶激活能Qr值为166.949~173.545 kJ.mol-1。 The microstructure evolution and static recrystallization kinetics at different annealing temperature ranged from 1 360 - 1 500 ℃ of forgingLa2O3-doped Mo alloy were researched. The experiment results demonstrated that the relationship between the annealing time and the fraction of recrystallization grains could be described by the J-M equation. Based on the kinetics analysis, the activation energy of recrystallization was calculated to be about 166. 949 -173. 545 kJ mol-1
出处 《上海金属》 CAS 北大核心 2012年第6期7-10,共4页 Shanghai Metals
关键词 掺杂La2O3 合金钼棒再结晶 动力学机制 再结晶激活能 La2O3-Doped Mo Alloy, Recrystallization, Kinetics Mechanism, Recrystal-lization Activation Energy
  • 相关文献

参考文献4

二级参考文献36

共引文献120

同被引文献12

引证文献2

二级引证文献3

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部