摘要 目的 通过对 Ti- 75合金铸造后挠度的测试分析 ,选择 Ti- 75合金临床应用的合理厚度 .方法 参照美国 ADA关于义齿基托树脂材料挠度的标准 ,对 Ti- 75合金的挠度进行了研究 ,并对 Ti及 Ti- 6 Al- 4V合金以及临床常用的 Co- Cr合金进行了对比研究 .结果  Ti- 75合金 ,纯钛及 Ti- 6 Al- 4V合金在厚度为 0 .6 5 m m左右时能够达到义齿基托挠度的标准 .钴铬合金在 0 .5 7mm左右时即可达到标准要求 .结论 在临床利用 Ti- 75合金制作基托时 ,厚度应选择 0 .6 5 AIM To explore the reasonable thickness of Ti 75 alloy used as denture base material. METHODS According to the 'revised ADA specification No. 12 for denture base polymers', the transverse deflection tests of Ti 75 alloy after casting were performed. Pure titanium, Ti 6Al 4V alloy and Co Cr alloy were used as control. RESULTS When the thickness was 0.65 mm for Ti 75 alloy, pure titanium and Ti 6Al 4V alloy, and 0.57 mm for Co Cr alloy, the transverse deflections could satisfy the requirement. CONCLUSION The reasonable thickness of Ti 75 alloy used as denture base material is 0.65 mm.
出处 《第四军医大学学报》 CAS 2000年第3期286-288,共3页 Journal of the Fourth Military Medical University
基金 国家自然科学基金资助项目!(39770805)
关键词 Ti-75合金 铸造 挠度 义齿基托 树脂材料 Ti-75 alloy transverse deflection
  • 相关文献

参考文献3

二级参考文献1

共引文献8

同被引文献14

引证文献1

二级引证文献8

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部