摘要 无铅焊料中添加硒可提高润湿性能,但硒不能直接添加到无铅焊料熔体中,需以Sn-Se中间合金形式添加,常规采用真空或惰性气体保护炉制备Sn-Se中间合金,但存在产生剧毒的二氧化硒和硒损耗大等诸多问题。本文探讨采用包裹挤压法制备Sn-Se中间合金,克服了现有技术的不足,研究表明该法设备投入少、操作容易、效果较好。 Selenium can improve the wetting properties for lead -free solder, but selenium can not be directly added to the lead - free solders melt, being added by the Sn - Se intermediate alloy. The conventional method prepares the intermediate alloys of Sn - Se is vacuum or inert gas protection furnace, but there is to produce highly toxic selenium dioxide and selenium great loss of many problems. This article explores the use of the parcel to squeeze the middle of Sn - Se alloy, overcoming the deficiencies of the existing technology. It shows that equipment costs lower, being easy to operate and the better of the Preparation Method.
出处 《有色金属加工》 CAS 2012年第6期16-17,24,共3页 Nonferrous Metals Processing
关键词 Sn—Se中间合金 包裹挤压法 Sn- Se intermediate alloy wrapping squeeze process
  • 相关文献

参考文献4

  • 1戴国水.无铅喷金材料的发展现状与展望[J].电子元件与材料,2008,27(10):1-4. 被引量:7
  • 2H.n.梁基谢夫.金属二元系相图手册[M].北京:化学工业出版社,2008.5.
  • 3陆文华.铸造合金及熔炼[M].北京:机械工业出版社1997.215-216.
  • 4刘正.一种镁锰中间合金及其制备方法[P].中国专利:03133459.8,2003-06-17.

二级参考文献11

共引文献10

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部