摘要 目的检测Bis-GMA/TEGDMA树脂片经去离子水浸泡后的水解产物。方法 Bis-GMA/TEGDMA单体加入CQ/DMAEMA后光照聚合制备树脂片,将树脂片经37℃恒温去离子水浸泡24 h,其中在1h、3 h、6 h和24 h四个时间点各取1 mL浸泡液,用乙酸乙酯萃取、旋蒸,通过高效液相色谱质谱法(HPLC/MS)检测分析,确定树脂水解产物。结果树脂片的水解产物为双酚A-二甘油醚(Bis-GMA-2MA)、双酚A-二氧代丙基醚(Bis-GMA-2MA-2H2O)、单甲基丙烯酸二缩三乙二醇酯(TEGDMA-MA)和二缩三乙二醇(TEGDMA-2MA)。结论 Bis-GMA/TEGDMA树脂片经去离子水浸泡后树脂可发生水解,水解产物及残余Bis-GMA/TEGDMA树脂单体可析出并释放到去离子水中。 Objective To detect the hydrolysis products of resin discs immersed in demonized water. Methods Light-cured resin discs composed of Bis-GMA/TEGDMA and CQ/DMAEMA were immersed in deionized water for 24 h at 37℃, then, 1 mL of soak Solution at 1 h, 3 h, 6 h and 24 h was extracted with ethyl acetate and evaporated by a rotary evaporator. Finally the hydrolysis products of resins were confirmed through the high performance liquid chromatography (HPLC) and mass spectrometry (MS). Results The hydrolysis products of Bis-GMA/TEGDMA resin discs were Bis- GMA-2MA, Bis-GMA-2MA-2H20, TEGDMA-MA and TEGDMA-2MA, respectively. Conclusions Bis-GMA/TEGDMA resin was hydrolyzed after immersed in deionized water. The hydrolysis products and residual monomers of Bis-GMA/ TEGDMA could be released into deionized water.
出处 《口腔材料器械杂志》 2012年第4期181-186,共6页 Chinese Journal of Dental Materials and Devices
基金 国家自然科学基金项目(30973356 81130078)
关键词 Bis—GMA TEGDMA树脂 水解 高效液相色谱质谱 Bis-GMA/TEGDMA resin Hydrolysis HPLC/MS
  • 相关文献

参考文献25

  • 1Ilie N, Hickel R. Resin composite restorative materials. Aust Dent J, 2011, 56(1) :59 -66.
  • 2Moraes RR, Garcia JW, Barros MD, et al. Control of polymerization shrinkage and stress in nanogel-modified monomer and composite materials. Dent Mater, 2011, 27 ( 6 ) : 509 - 519.
  • 3Ferracane JK. Resin composite--state of the art. Dent Mater, 2011, 27(1) :29 -38.
  • 4Nishiyama N, Tay FR, Fujita K, et al. Hydrolysis of functional monomers in a single-bottle self-etching primer--correlation of 13C NMR and TEM findings. J Dent Res, 2006, 85(5) :422 -426.
  • 5Polydorou O, Tr/tt|er R, Hellwig E, et al. Elution of monomers from two conventional dental composite materials. Dent Mater, 2007, 23 (12) :1535 - 1541.
  • 6Uzunova Y, Uzunova L, Filipov I, et al. High-performance liquid chromatographic determination of unreacted monomers and other residues contained in dental composites. J Biochem Biophys Methods, 2008, 70(6):883-888.
  • 7Michelse VB, Lygrc H, Skalevik R, et al. Identification of organic eluates from four polymer-based dental filling materials. Eur J Oral Sci, 2003, 111 (3) :263 - 271.
  • 8Zhou MS, Wu CP, Edirisinghe PD, et al. Organic overlayer model of a dental composite analyzed by laser desorption postionization mass spectrometry and photoemission. J Biomed Mater Res A, 2006, 77(1) :1 - 10.
  • 9Hashimoto M, Nagano F, Endo K, et al. A review: Biodegradation of resin-dentin bonds. JDSR, 2011,77( 1 ) :5 - 12.
  • 10Santerre JP, Shajii L, Lenng BW..Relation of dental composite formulations to their degradation and the release of hydrolyzed polymer/c-resin-derived products. Crit Rev Oral Biol Med, 2001, 12(2) :136 N 151.

同被引文献16

  • 1朱雅红,马晓燕,陈娜.聚合物基复合材料的界面及改性研究[J].玻璃钢/复合材料,2005(3):44-48. 被引量:11
  • 2Goracci C,Ferrari M.Current perspectives on post systems:a literature review[J].Aust Dent J,2011,56(suppl 1):77-83.
  • 3Chieruzzi M,Pagano S,Pennacchi M,et al.Compressive and flexural behaviour of fibre reinforced endodonticposts[J].J Dent,2012,40(11):968-978.
  • 4Sun L,Jia Y,Ma F,et al.Influence of interfacial properties on crack propagation in fiber-reinforced polymer matrix composites[J].Macro Mater and Engineer,2008,293(3):194-205.
  • 5Li HZ,Jia YX,Wan SF,et al.Influence of inter-fiber spacing and interfacial adhesion on failure of multi-fiber model composites:Experiment and numerical analysis[J].Polymer Composites,2008,29(9):964-71.
  • 6Liu FW,Wang RL,Cheng YH,et al.Polymer grafted hydroxyapatite whisker as a filler for dental composite resin with enhanced physical and mechanical properties[J].Mater Sci and Eng C Mater Biol Appl,2013,33(8):4994-5000.
  • 7International Organization for Standardization.10477:1992(E)I.Dentistry.Polymer based crown and bridgematerials[S].Switzerland:Geneva,1992.
  • 8Pegoretti A,Fambri L,Zappini G,et al.Finite element analysis of a glass fibre reinforced composite endodontic post[J].Biomaterials,2002,23(13):2667-82.
  • 9Zhang M,Matinlinna JP.E-glass fiber reinforced composites in dental applications[J].Silicon,2012,4(1):73-78.
  • 10Wang RL,Liu FW,Wang SC,et al.Surface modification of quartz fibre and its reinforced bis-GMA/MMA composites for dental post[C].Qingdao:C-MRS&IUMRS,2013.

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部