基准砂浆抗渗性能检测结果稳定性的探讨和研究 被引量:1

Discussion and Study on Stability of Impermeability Test Results for Fiducial Mortar
下载PDF
导出
摘要 在实验室条件下,通过调整砂浆配合比,采用不同的密实方法、养护手段,掺入外加剂等方式来制备多组基准砂浆试件,并测试其养护至7 d龄期时的透水压力值,目的是寻找合适的配比和方法,使基准砂浆的透水压力值能稳定在0.3~0.5 MPa,以满足各种防水材料性能检测的要求。结果表明,水泥:砂:水:纤维素醚=360:1 350:220:0.5,采用手工插捣密实,浸水养护或入养护箱养护的砂浆试件抗渗性能均较为稳定,且满足检测要求。 Fiducial mortar samples with different mixture ratios were prepared by different compaction methods, curing methods, and additive. The permeability of the samples after 7 days of curing was determined so as to find a suitable mixture ratio and method that make the samples can resist the water pressure among 0.3-0.5 MPa, which meets the requirement of performance tests for waterproofing materials. The results showed the suitable mixture ratio was cement:sand:water:cellulose ether =360:1 350:220:0.5, the proper compaction method was hand pudding, and the optimum curing method was curing in water or box.
出处 《中国建筑防水》 2013年第1期35-38,45,共5页 China Building Waterproofing
关键词 基准砂浆 透水压力 抗渗压力 配合比 密实方法 养护 外加剂 fiducial mortar seepage pressure impermeability pressure mixture ratio compaction method curing additive
  • 相关文献

参考文献7

  • 1全国水泥制品标准化技术委员会.JC474-2008砂浆、混凝土防水剂[S].北京:中国建材工业出版社,2008.
  • 2全国水泥制品标准化技术委员会.GB23440-2009无机防水堵漏材料[S].北京:中国标准出版社,2009.
  • 3全国轻质与装饰装修建筑材料标准化技术委员会.GB/T23445--2009聚合物水泥防水涂料[s].北京:中国标准出版社.2009.
  • 4全国水泥标准化技术委员会.GB/T17671-1999水泥胶砂强度检验方法(ISO法)[S].北京:中国标准出版社,1999.
  • 5全国水泥标准化技术委员会.GB/T2419-2005水泥胶砂流动度测定方法[S].北京:中国标准出版社,2005.
  • 6全国轻质与装饰装修建筑材料标准化技术委员会.JC887-2001干挂石材幕墙用环氧胶粘剂[S].北京:中国建材工业出版社,2002.
  • 7刘军,刘淑英,陈集阳,李春.水泥基渗透结晶型防水材料抗渗性能检测方法的探讨[J].河南建材,2005(4):46-47. 被引量:1

二级参考文献3

共引文献4

同被引文献6

引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部