摘要 介绍了采用回转窑—电炉法(RKEF)处理缅甸达贡山镍红土矿生产镍铁的中试试验过程,得到了下述最佳工艺参数:干燥后原矿含水20%~22%、回转窑预还原温度900℃、还原剂煤的配入量7%、镍品位19%,烟尘制粒时湿矿配入量为烟尘的25%、尘球含水30%,电炉熔炼时放渣温度1 550~1 600℃、镍铁合金放出温度1 450~1 500℃。 The pilot plant test on ferronickel alloy production from Myanmar Dagon Hill nickel laterite by rotary kiln-electric furnace smelting process (RKEF) was introduced. The optimum process parameters in- clude moisture of 20-22% in dried ore, pre-reduction temperature of 900 ℃, reductant dosage of 7%, nickel grade in ferronickel alloy of 19%; 25% of dust as dosage of wet laterite, the moisture of dustball of 30% in palletizing process, slag and ferronickel alloy discharging temperature in electric furnace smelting process of 1 550-1 600 ℃ and 1 450-1500 ℃, respectively.
作者 赵景富
出处 《有色金属(冶炼部分)》 CAS 北大核心 2013年第1期8-10,16,共4页 Nonferrous Metals(Extractive Metallurgy)
关键词 镍红土矿 干燥 还原焙烧 镍铁合金 制粒 回转窑 电炉 nickel laterite drying reduction roasting ferronickel alloy pelletizing rotary kiln electric furnace
  • 相关文献

参考文献5

二级参考文献17

共引文献93

同被引文献101

引证文献11

二级引证文献57

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部