通过试验研究出铝合金5182-O态生产工艺为:均匀化退火温度470℃,再结晶终了温度280℃。在试验条件下,产品力学性能和成形性能达到国标要求。
The production technology of aluminum alloy 5182-O states was developed: the homogenizing annealing temperature is 470 ℃. The recrystallization temperature is 280 ℃. Under the experimental conditions, the mechanical properties and formability of the product can achieve the requirements of standard.