摘要
以米糠为原料,用5%氢氧化钾液煮沸浸泡30min处理后,形成pH小于3.3,比表面积13m2/g,大孔体积35.5mL/g二氧化硅沉淀吸附剂即改性米糠。本文研究了利用该改性米糠去除回收磷酸液中铁离子的最佳条件。实验结果表明:在常温下,改性米糠3g与磷酸液中的铁离子接触24h,过滤,即可达到除铁的目的,用此法除铁离子效果可达90%,是一种值得推广的应用技术。
Using Rice bran as a raw material, after 30rain treatment of a 5% potassium hydroxide solution to boil soak, it becomes a pH≤3.3, the surface area 13m2 / g, the macropore volume of 35.5 ml / g silica precipitation adsorbent i.e. modified rice bran. This paper studied the best condition of using this modified rice bran to remove iron ion in the recovered phosphoric acid solution. Experiment result showed that at room temperature, 3g of the modified rice bran contacted with the iron ions in the phosphoric liquid 24h, filtered, then the purpose of the removal of iron is achieved, the efficiency of this method is up to 90%.This method is a worthy application technology.
出处
《质量技术监督研究》
2012年第5期30-32,共3页
Quality and Technical Supervision Research
基金
南平市科技局项目课题[N2010D05]
关键词
米糠
氢氧化钾
二氧化硅沉淀吸附剂
铁离子
Nice husk
Potassium hydroxide
Silica precipitation adsorbent
Ferric ion