摘要
在连续升温过程中 ,测量了Pb Sn合金的内耗 .实验发现 :在共晶成分范围内 ,伴随着Pb Sn合金的固—液转变 ,内耗值出现突然下降 .内耗值的下降幅度与Pb Sn合金成分有关 .固—液转变过程中的内耗是由材料结构变化或弛豫时间变化引起的 .
The internal friction of the Pb\|Sn alloys was measured during heating process from room temperature to high temperature.It is reported that there is a sudden drop in the internal friction curves of the vibration systems with the presence of solid\|liquid transition of the Pb\|Sn alloys.The decrement of the internal friction varies with the content of tin.It is proposed that these variations are related with the structure variation of the Pb\|Sn alloys during solid-liquid transition.
出处
《物理学报》
SCIE
EI
CAS
CSCD
北大核心
2000年第7期1327-1330,共4页
Acta Physica Sinica
基金
国家自然科学基金! (批准号 :198740 67)
中国科学院"九五"基础研究重大项目基金! (批准号 :KJ 95 2 J1 412 )
关键词
内耗
固-液转变
PB-SN合金
internal friction, solid-liquid transition, Pb\|Sn alloy