摘要
研究了用 Na Cl O浸取低品位钼精矿及用 NH4 Cl从浸取液中沉淀钼的工艺条件。钼的总回收率不低于 94% ,产品 Mo O3 中的钼含量不低于 57%。
It has been studied for the conditions of the process that molybdenite is leached with NaClO and molybdate is precipitated from the solution with NH 4Cl.The total recovery rate of molybdenum is up to 94%. The content of molybdate in MoS 3 over 57%.
出处
《新技术新工艺》
北大核心
2000年第6期27-28,共2页
New Technology & New Process