摘要 采用R型铂铑合金热电偶的方法测量硅系延期药的燃烧温度,模拟单芯延期体的燃烧状况,将延期药以2.40 g/cm3的压药密度,分次均匀压入厚壁钢管中。在热量积累最多的区域内,实验测得硅系延期药的最高燃烧温度为1583℃。燃烧热有很大部分传递给外壳等物质而散失掉,35ms后测出的温度较低。 Pt-Rh thermocouple is used to measure combustion temperature of silicon delay-composition. The combus- tion state of singe delay composition is simulated, and the delay composition is loaded in a steel thick tube by several times with the density is 2.40g/cm3. The highest measured temperature is 1583℃ at the mainly heat-accumulation area. Most of the combustion heat loses in the transmission to the shells and so on, and the much lower temperature is measured after 35ms.
作者 宋薇娜
出处 《爆破器材》 CAS 北大核心 2013年第2期41-43,共3页 Explosive Materials
关键词 热电偶 硅系延期药 燃烧温度 燃烧状态 thermoeouple, silicon delay composition, combustion temperature, combustion state
  • 相关文献

参考文献5

二级参考文献26

  • 1王志朋,劳允亮.钨系延期药预点火反应机理研究[J].火工品,1996(4):19-22. 被引量:12
  • 2张克林,刘自汤,汤明钧,彭金华.塑料导爆管点燃延期药的初步探讨[J].爆破器材,1989,18(5):1-3. 被引量:4
  • 3阚金玲,刘家骢,曾秀琳,王静.温压炸药爆炸火球的特征[J].火炸药学报,2007,30(2):55-58. 被引量:20
  • 4煤矿火工技术丛书编写组.矿用起爆材料[M].北京:煤炭工业出版社,1977.246.
  • 5史山群.国外火工品[M].北京:国防工业出版社,1977.42-54.
  • 6Honzinger,Walter,etc. Pyrotechnical delay composition. USP4776275,Oct. 11,1988.
  • 7Hidetsugu N, Miyako A, Yasutake H. The combustion mechanism of tungsten-potassium perchlorate-barium chromate delay powder[J]. Kayaku Gakkaishi,2000,61 ( 1 ):7 -12.
  • 8McLain J H. Pyrotecgbucs from the Viewpoint of Solid State Chemistry[ M ]. The Franklin Institute Press, 1980.
  • 9Jun Z,Yun-liang L,Cong-zhang Z. The mechanism of solid state reaction of silicon and red lead delay composition[A]. 17th Proc. Int. Pyrotech. Seminar [C],1991,176- 182.
  • 10黄浩川.兵器工业科学技术辞典·火工品与烟火技术[M].北京:国防工业出版社,1992..

共引文献87

同被引文献22

引证文献3

二级引证文献5

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部