摘要
在钢管焊接检测中,真实反映焊缝中的缺陷性质有助于优化焊接工艺,降低材料损耗,提高生产效率。A型超声波探伤仪在埋弧焊钢管焊缝检测过程中只能反映缺陷的位置和大小,而对缺陷性质的判定存在一定的困难。通过对焊缝加工工艺,缺陷几何位置和缺陷静、动态波形等几个方面的研究和综合分析,总结出了埋弧焊钢管焊缝中存在的裂纹、未焊透、未熔合、夹渣和气孔等缺陷性质的评定方法。
During steel pipe wehling detection, really reflect defect nalure of weld is helpful to optimizing welding porocess, decreasing material wastage, anti increasing production efficiency. At present, The A-type ultrasonic flaw detector only can reflect the Iocation and size of defect, while it is difficult to delerrnine defect nature. In this article, it canrried out comprehensive analysis from severn) aspects, such as proeessing teehnology of wehl, geometrie posilhm of weld, stalie and dynamic waveform of wehl. and so on, smnmarized assessment method to crack, incomplete penetralion, incomplete fusion, slag inclusion , gas pocket and other defects existed in SAW pipe weld.
出处
《焊管》
2013年第4期53-56,共4页
Welded Pipe and Tube
关键词
A型超声波探伤仪
埋弧焊缝
焊缝缺陷
评定方法
A-type ultrasonic flaw detector
submerged arc weld
weld defect
assessment method