摘要
介绍了采用覆砂铁型铸造生产火车用摩擦斜楔ADI铸件的铸造工艺和热处理工艺。通过采用半封闭式浇注系统和过滤网挡渣;选用合理的炉料配比及喂丝球化处理工艺;采用盐浴等温淬火工艺,最终获得以贝氏体+残余奥氏体为基体的高强度、高硬度及高韧性的ADI铸件。
The casting method and heat treatment proeess adopted for using resin sand coated-iron mold to produce ADI oblique wedge of railway vehicles was introduced. By adopting semi-pressurized gating system and filter to skim slag, choosing rational mehing charge mixture ratio and the cored-wire injection nodularizing process, using salt bath isothermal quenching process, the hi-strength , hi-hardness and hi-toughness ADI castings with bainite + residual auslenite as matrix were finally obtained.
出处
《现代铸铁》
CAS
2013年第2期33-36,共4页
Modern Cast Iron
关键词
ADI
覆砂铁型
喂丝球化处理法
ADI
resin sand euated-iron mold
eored-wire injection nodularizing process